Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.62 g/cm³ Show Supplier Material materials with Dichte of 1.62 g/cm³ | dry | ISO 1183 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 11.5 GPa Show Supplier Material materials with Biegemodul of 11.5 GPa | dry | ISO 178 | |
Dehnung | 2.5 % Show Supplier Material materials with Dehnung of 2.5 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 12.5 GPa Show Supplier Material materials with Elastizitätsmodul of 12.5 GPa | dry | ISO 527-1/-2 | |
Flexural yield strength | 285 MPa Show Supplier Material materials with Flexural yield strength of 285 MPa | dry | ISO 178 | |
Schlagfestigkeit, Charpy gekerbt | 23 °C | 11 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 11 kJ/m² | dry | ISO 179/1eA |
Schlagzähigkeit, Charpy ungekerbt | 23 °C | 60 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 60 kJ/m² | dry | ISO 179/1eU |
Zugfestigkeit | 200 MPa Show Supplier Material materials with Zugfestigkeit of 200 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Glasübergangstemperatur | 75 °C Show Supplier Material materials with Glasübergangstemperatur of 75 °C | dry | ISO 11357-1/-2 | 10°C/min | ||
Koeffizient der thermischen Ausdehnung | 2.5e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
5.3e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 5.3e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | dry | UL746B | 3 mm | ||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | UL746B | 3 mm | ||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | dry | UL746B | 3 mm | ||
Wärmeformbeständigkeitstemperatur | 270 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 270 °C | dry | ISO 75-1/-2 | 2 MPa |
Elektrisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Kriechstromfestigkeit | 200 V Show Supplier Material materials with Kriechstromfestigkeit of 200 V | dry | IEC 60112 |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available | |
Fillers | 33% Glass Fiber |