Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.13 g/cm³ Show Supplier Material materials with Dichte of 1.13 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.8 % Show Supplier Material materials with Moisture absorption of 2.8 % | dry | Sim. to ISO 62 |
Wasserabsorption | 9 % Show Supplier Material materials with Wasserabsorption of 9 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Dehnung | 35 % Show Supplier Material materials with Dehnung of 35 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 3.3 GPa Show Supplier Material materials with Elastizitätsmodul of 3.3 GPa | dry | ISO 527-1/-2 | |
Elongation at yield | 4 % Show Supplier Material materials with Elongation at yield of 4 % | dry | ISO 527-1/-2 | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 4 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 4 kJ/m² | dry | ISO 179/1eA |
23 °C | 7 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 7 kJ/m² | dry | ISO 179/1eA |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 1e-06 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1e-06 1/K | dry | ISO 11359-1/-2 | Parallel | |
1.4e-06 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.4e-06 1/K | dry | ISO 11359-1/-2 | Normal | ||
Schmelzpunkt | 220 °C Show Supplier Material materials with Schmelzpunkt of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Wärmeformbeständigkeitstemperatur | 60 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 60 °C | dry | ISO 75-1/-2 | 2 MPa | |
150 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 150 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Rheological Properties
Property | Value | Condition | Testing Standard |
---|---|---|---|
Viscosity number | 195 cm³/gr Show Supplier Material materials with Viscosity number of 195 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property |
---|