Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dichte | 1.18 g/cm³ Show Supplier Material materials with Dichte of 1.18 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 3 % Show Supplier Material materials with Moisture absorption of 3 % | dry | Sim. to ISO 62 | |
Wasserabsorption | 3.1 % Show Supplier Material materials with Wasserabsorption of 3.1 % | dry | ISO 62 | at 23°C after 24h |
11.5 % Show Supplier Material materials with Wasserabsorption of 11.5 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Dehnung | 10 % Show Supplier Material materials with Dehnung of 10 % | dry | ISO 527-1/-2 | |
120 °C | 24 % Show Supplier Material materials with Dehnung of 24 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 3.7 GPa Show Supplier Material materials with Elastizitätsmodul of 3.7 GPa | dry | ISO 527-1/-2 | |
120 °C | 1.4 GPa Show Supplier Material materials with Elastizitätsmodul of 1.4 GPa | dry | ISO 527-1/-2 | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 5 kJ/m² | dry | ISO 179/1eA |
23 °C | 12 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 12 kJ/m² | dry | ISO 179/1eA | |
Zugfestigkeit | 95 MPa Show Supplier Material materials with Zugfestigkeit of 95 MPa | dry | ISO 527-1/-2 | |
120 °C | 50 MPa Show Supplier Material materials with Zugfestigkeit of 50 MPa | dry | ISO 527-1/-2 |
Thermisch
Technological properties
Property | ||
---|---|---|
Fillers | 8% Glass Fiber |