Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.24 g/cm³ Show Supplier Material materials with Dichte of 1.24 g/cm³ | dry | ISO 1183 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Dehnung | 2.5 % Show Supplier Material materials with Dehnung of 2.5 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 5.5 GPa Show Supplier Material materials with Elastizitätsmodul of 5.5 GPa | dry | ISO 527-1/-2 | |
Schlagfestigkeit, Charpy gekerbt | 23 °C | 6 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 6 kJ/m² | dry | ISO 179/1eA |
Schlagzähigkeit, Charpy ungekerbt | 23 °C | 35 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 35 kJ/m² | dry | ISO 179/1eU |
Zugfestigkeit | 115 MPa Show Supplier Material materials with Zugfestigkeit of 115 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Schmelzpunkt | 220 °C Show Supplier Material materials with Schmelzpunkt of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Temperaturleitfähigkeit | 1.12e-07 mm²/s Show Supplier Material materials with Temperaturleitfähigkeit of 1.12e-07 mm²/s | dry | - | ||
Wärmeformbeständigkeitstemperatur | 190 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 190 °C | dry | ISO 75-1/-2 | 2 MPa | |
210 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 210 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Density of melt | 1150 g/cm³ Show Supplier Material materials with Density of melt of 1150 g/cm³ | dry | - | ||
Schmelzvolumenflussrate | 235 °C | 23 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 23 cm³/10min | dry | ISO 1133 | |
Schrumpfung | 0.5 % Show Supplier Material materials with Schrumpfung of 0.5 % | dry | ISO 294-4 | Parallel | |
0.9 % Show Supplier Material materials with Schrumpfung of 0.9 % | dry | ISO 294-4 | Normal | ||
Specific heat capacity melt | 2110 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 2110 J/(kg·K) | dry | - | ||
Thermal conductivity of melt | 0.27 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.27 W/(m·K) | dry | - |
Technological properties
Property | ||
---|---|---|
Fillers | 15% Glass Fiber |