Allgemein
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dichte | 1.26 g/cm³ Show Supplier Material materials with Dichte of 1.26 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 3.2 % Show Supplier Material materials with Moisture absorption of 3.2 % | dry | Sim. to ISO 62 | |
Wasserabsorption | 3.3 % Show Supplier Material materials with Wasserabsorption of 3.3 % | dry | ISO 62 | at 23°C after 24h |
11.4 % Show Supplier Material materials with Wasserabsorption of 11.4 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 2.9 GPa Show Supplier Material materials with Biegemodul of 2.9 GPa | dry | ISO 178 | |
Dehnung | -40 °C | 9 % Show Supplier Material materials with Dehnung of 9 % | dry | ISO 527-1/-2 |
25 % Show Supplier Material materials with Dehnung of 25 % | dry | ISO 527-1/-2 | ||
50 % Show Supplier Material materials with Dehnung of 50 % | conditioned | ISO 527-1/-2 | ||
100 °C | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-1/-2 | |
120 °C | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-1/-2 | |
160 °C | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-1/-2 | |
180 °C | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-1/-2 | |
200 °C | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | -40 °C | 3.5 GPa Show Supplier Material materials with Elastizitätsmodul of 3.5 GPa | dry | ISO 527-1/-2 |
0.9 GPa Show Supplier Material materials with Elastizitätsmodul of 0.9 GPa | conditioned | ISO 527-1/-2 | ||
3.1 GPa Show Supplier Material materials with Elastizitätsmodul of 3.1 GPa | dry | ISO 527-1/-2 | ||
100 °C | 0.86 GPa Show Supplier Material materials with Elastizitätsmodul of 0.86 GPa | dry | ISO 527-1/-2 | |
120 °C | 0.77 GPa Show Supplier Material materials with Elastizitätsmodul of 0.77 GPa | dry | ISO 527-1/-2 | |
140 °C | 0.7 GPa Show Supplier Material materials with Elastizitätsmodul of 0.7 GPa | dry | ISO 527-1/-2 | |
160 °C | 0.65 GPa Show Supplier Material materials with Elastizitätsmodul of 0.65 GPa | dry | ISO 527-1/-2 | |
180 °C | 0.6 GPa Show Supplier Material materials with Elastizitätsmodul of 0.6 GPa | dry | ISO 527-1/-2 | |
200 °C | 0.56 GPa Show Supplier Material materials with Elastizitätsmodul of 0.56 GPa | dry | ISO 527-1/-2 | |
Elongation at yield | 17 % Show Supplier Material materials with Elongation at yield of 17 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 120 MPa Show Supplier Material materials with Flexural yield strength of 120 MPa | dry | ISO 178 | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 6 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 6 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 9 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 9 kJ/m² | dry | ISO 179/1eA | |
23 °C | 15 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 15 kJ/m² | conditioned | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 150 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 150 kJ/m² | dry | ISO 179/1eU |
Streckgrenze | 50 MPa Show Supplier Material materials with Streckgrenze of 50 MPa | conditioned | ISO 527-1/-2 | |
90 MPa Show Supplier Material materials with Streckgrenze of 90 MPa | dry | ISO 527-1/-2 | ||
100 °C | 50 MPa Show Supplier Material materials with Streckgrenze of 50 MPa | dry | ISO 527-1/-2 | |
120 °C | 45 MPa Show Supplier Material materials with Streckgrenze of 45 MPa | dry | ISO 527-1/-2 | |
160 °C | 40 MPa Show Supplier Material materials with Streckgrenze of 40 MPa | dry | ISO 527-1/-2 | |
180 °C | 35 MPa Show Supplier Material materials with Streckgrenze of 35 MPa | dry | ISO 527-1/-2 | |
200 °C | 30 MPa Show Supplier Material materials with Streckgrenze of 30 MPa | dry | ISO 527-1/-2 | |
Zugfestigkeit | -40 °C | 115 MPa Show Supplier Material materials with Zugfestigkeit of 115 MPa | dry | ISO 527-1/-2 |
55.0 MPa Show Supplier Material materials with Zugfestigkeit of 55.0 MPa | conditioned | ISO 527-1/-2 | ||
85 MPa Show Supplier Material materials with Zugfestigkeit of 85 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Glasübergangstemperatur | 75 °C Show Supplier Material materials with Glasübergangstemperatur of 75 °C | dry | ISO 11357-1/-2 | 10°C/min | |
Koeffizient der thermischen Ausdehnung | 8.5e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 8.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
1.1e-06 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.1e-06 1/K | dry | ISO 11359-1/-2 | Normal | ||
Schmelzpunkt | 295 °C Show Supplier Material materials with Schmelzpunkt of 295 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Vicat-Erweichungstemperatur | 290 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 290 °C | dry | ISO 306 | 50°C/h 50N | |
Wärmeformbeständigkeitstemperatur | 190 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 190 °C | dry | ISO 75-1/-2 | 2 MPa | |
290 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 290 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schrumpfung | 2 % Show Supplier Material materials with Schrumpfung of 2 % | dry | Sim. to ISO 294-4 | Parallel |
2 % Show Supplier Material materials with Schrumpfung of 2 % | dry | Sim. to ISO 294-4 | Normal | |
Spiral flow length | 115 | dry | - | 1.0 mm 800 bar |
125 | dry | - | 1.0 mm 900 bar | |
135 | dry | - | 1.0 mm 1000 bar | |
Viscosity number | 190 cm³/gr Show Supplier Material materials with Viscosity number of 190 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Application areas | Slide Shoe Surfaces in new generation, New Generation Slide Shoe Surfaces, Timing drive systems | |
Fillers | PTFE |