Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Bio-based content | 70 % Show Supplier Material materials with Bio-based content of 70 % | dry | ASTM D6866-12 Method B |
Dichte | 1.34 g/cm³ Show Supplier Material materials with Dichte of 1.34 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.5 % Show Supplier Material materials with Moisture absorption of 1.5 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 6.3 GPa Show Supplier Material materials with Biegemodul of 6.3 GPa | conditioned | ISO 178 | |
8.5 GPa Show Supplier Material materials with Biegemodul of 8.5 GPa | dry | ISO 178 | ||
120 °C | 4.8 GPa Show Supplier Material materials with Biegemodul of 4.8 GPa | dry | ISO 178 | |
Dehnung | 3.8 % Show Supplier Material materials with Dehnung of 3.8 % | dry | ISO 527-1/-2 | |
5.8 % Show Supplier Material materials with Dehnung of 5.8 % | conditioned | ISO 527-1/-2 | ||
120 °C | 8.2 % Show Supplier Material materials with Dehnung of 8.2 % | dry | ISO 527-1/-2 | |
160 °C | 9.4 % Show Supplier Material materials with Dehnung of 9.4 % | dry | ISO 527-1/-2 | |
180 °C | 10 % Show Supplier Material materials with Dehnung of 10 % | dry | ISO 527-1/-2 | |
200 °C | 10 % Show Supplier Material materials with Dehnung of 10 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 7 GPa Show Supplier Material materials with Elastizitätsmodul of 7 GPa | conditioned | ISO 527-1/-2 | |
9.2 GPa Show Supplier Material materials with Elastizitätsmodul of 9.2 GPa | dry | ISO 527-1/-2 | ||
120 °C | 4.6 GPa Show Supplier Material materials with Elastizitätsmodul of 4.6 GPa | dry | ISO 527-1/-2 | |
160 °C | 3.7 GPa Show Supplier Material materials with Elastizitätsmodul of 3.7 GPa | dry | ISO 527-1/-2 | |
180 °C | 3.2 GPa Show Supplier Material materials with Elastizitätsmodul of 3.2 GPa | dry | ISO 527-1/-2 | |
200 °C | 3 GPa Show Supplier Material materials with Elastizitätsmodul of 3 GPa | dry | ISO 527-1/-2 | |
Flexural yield strength | 185 MPa Show Supplier Material materials with Flexural yield strength of 185 MPa | conditioned | ISO 178 | |
260 MPa Show Supplier Material materials with Flexural yield strength of 260 MPa | dry | ISO 178 | ||
120 °C | 145 MPa Show Supplier Material materials with Flexural yield strength of 145 MPa | dry | ISO 178 | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 9 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 9 kJ/m² | dry | ISO 179/1eA |
23 °C | 11 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 11 kJ/m² | dry | ISO 179/1eA | |
23 °C | 15 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 15 kJ/m² | conditioned | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 60 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 60 kJ/m² | dry | ISO 179/1eU |
23 °C | 80 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 80 kJ/m² | dry, conditioned | ISO 179/1eU | |
Zugfestigkeit | 115 MPa Show Supplier Material materials with Zugfestigkeit of 115 MPa | conditioned | ISO 527-1/-2 | |
170 MPa Show Supplier Material materials with Zugfestigkeit of 170 MPa | dry | ISO 527-1/-2 | ||
120 °C | 85 MPa Show Supplier Material materials with Zugfestigkeit of 85 MPa | dry | ISO 527-1/-2 | |
160 °C | 70 MPa Show Supplier Material materials with Zugfestigkeit of 70 MPa | dry | ISO 527-1/-2 | |
180 °C | 65 MPa Show Supplier Material materials with Zugfestigkeit of 65 MPa | dry | ISO 527-1/-2 | |
200 °C | 60 MPa Show Supplier Material materials with Zugfestigkeit of 60 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 3.2e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 3.2e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
6.6e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 6.6e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Schmelzpunkt | 250 °C Show Supplier Material materials with Schmelzpunkt of 250 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Wärmeformbeständigkeitstemperatur | 215 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 215 °C | dry | ISO 75-1/-2 | 2 MPa | |
243 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 243 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Elektrisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Surface resistivity | 1e+13 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+13 Ω/sq | conditioned | IEC 62631-3-2 |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | conditioned | IEC 62631-3-1 |
1e+12 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+12 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Schmelzmassenflussrate | 290 °C | 42 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 42 g/10min | dry | ISO 1133 | |
Schmelzvolumenflussrate | 290 °C | 36 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 36 cm³/10min | dry | ISO 1133 | |
Schrumpfung | 0.5 % Show Supplier Material materials with Schrumpfung of 0.5 % | dry | ISO 294-4 | Parallel | |
1 % Show Supplier Material materials with Schrumpfung of 1 % | dry | ISO 294-4 | Normal |
Technological properties
Property | ||
---|---|---|
Application areas | Window profiles, Snowboard bindings, Mountaineering shoes, Coolant Hose T-Connectors, Charge Air Cooler Caps, Fuel System: Various Components, Fuel Line Connectors, Automotive Connectors, Temperature Sensor, Speed Sensor, Positition Sensor, Wheel Speed Sensors, Coolant expansion tank, Radiator end tanks, Coolant connectors | |
Fillers | 30% Glass Fiber |