Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.16 g/cm³ Show Supplier Material materials with Dichte of 1.16 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.4 % Show Supplier Material materials with Moisture absorption of 0.4 % | dry | Sim. to ISO 62 |
Wasserabsorption | 7 % Show Supplier Material materials with Wasserabsorption of 7 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Biegemodul | 0.04 GPa Show Supplier Material materials with Biegemodul of 0.04 GPa | dry | ISO 178 | |
Dehnung | 450 % Show Supplier Material materials with Dehnung of 450 % | dry | ISO 527-1/-2 | |
810 % Show Supplier Material materials with Dehnung of 810 % | dry | ISO 527-1/-2 | ||
Elastizitätsmodul | 0.05 GPa Show Supplier Material materials with Elastizitätsmodul of 0.05 GPa | dry | ISO 527-1/-2 | |
Härte, Shore D | 32 [-] Show Supplier Material materials with Härte, Shore D of 32 [-] | dry | ISO 868 | 3s |
Reißfestigkeit | 93 kN/m Show Supplier Material materials with Reißfestigkeit of 93 kN/m | dry | ISO 34-1; Method B | |
95 kN/m Show Supplier Material materials with Reißfestigkeit of 95 kN/m | dry | ISO 34-1; Method B | ||
Zugfestigkeit | 14.0 MPa Show Supplier Material materials with Zugfestigkeit of 14.0 MPa | dry | ISO 527-1/-2 | |
18 MPa Show Supplier Material materials with Zugfestigkeit of 18 MPa | dry | ISO 527-1/-2 | Normal |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 1.5e-06 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.5e-06 1/K | dry | ISO 11359-1/-2 | Parallel |
1.5e-06 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.5e-06 1/K | dry | ISO 11359-1/-2 | Normal | |
Schmelzpunkt | 212 °C Show Supplier Material materials with Schmelzpunkt of 212 °C | dry | ISO 11357-1/-3 | 10°C/min |
Vicat-Erweichungstemperatur | 124 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 124 °C | dry | ISO 306 | 50°C/h 10N |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 4.4 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4.4 [-] | dry | IEC 62631-2-1 | 1MHz |
4.7 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4.7 [-] | dry | IEC 62631-2-1 | 100Hz | |
Durchschlagfestigkeit | 20 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 20 kV/mm | dry | IEC 60243-1 | |
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | dry | IEC 60112 | |
Verlustfaktor | 310 [-] Show Supplier Material materials with Verlustfaktor of 310 [-] | dry | IEC 62631-2-1 | 100Hz |
810 [-] Show Supplier Material materials with Verlustfaktor of 810 [-] | dry | IEC 62631-2-1 | 1MHz | |
Volume resistivity | 1e+12 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+12 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Schmelzvolumenflussrate | 230 °C | 32 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 32 cm³/10min | dry | ISO 1133 | |
Schrumpfung | 1.55 % Show Supplier Material materials with Schrumpfung of 1.55 % | dry | ISO 294-4 | Parallel | |
1.75 % Show Supplier Material materials with Schrumpfung of 1.75 % | dry | ISO 294-4 | Normal |
Technological properties
Property | ||
---|---|---|
Application areas | Body Plugs |