Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.56 g/cm³ Show Supplier Material materials with Dichte of 1.56 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.4 % Show Supplier Material materials with Moisture absorption of 1.4 % | dry | Sim. to ISO 62 |
Wasserabsorption | 4.5 % Show Supplier Material materials with Wasserabsorption of 4.5 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 16 GPa Show Supplier Material materials with Biegemodul of 16 GPa | dry | ISO 178 | |
Dehnung | 3 % Show Supplier Material materials with Dehnung of 3 % | dry | ISO 527-1/-2 | |
3.5 % Show Supplier Material materials with Dehnung of 3.5 % | conditioned | ISO 527-1/-2 | ||
Elastizitätsmodul | 12 GPa Show Supplier Material materials with Elastizitätsmodul of 12 GPa | conditioned | ISO 527-1/-2 | |
16 GPa Show Supplier Material materials with Elastizitätsmodul of 16 GPa | dry | ISO 527-1/-2 | ||
Flexural yield strength | 360 MPa Show Supplier Material materials with Flexural yield strength of 360 MPa | dry | ISO 178 | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 15 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 15 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 22 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 22 kJ/m² | dry | ISO 179/1eA | |
23 °C | 25 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 25 kJ/m² | conditioned | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 85 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 85 kJ/m² | dry, conditioned | ISO 179/1eU |
23 °C | 100 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 100 kJ/m² | dry | ISO 179/1eU | |
23 °C | 105 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 105 kJ/m² | conditioned | ISO 179/1eU | |
Zugfestigkeit | 160 MPa Show Supplier Material materials with Zugfestigkeit of 160 MPa | conditioned | ISO 527-1/-2 | |
230 MPa Show Supplier Material materials with Zugfestigkeit of 230 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Thickness | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|---|
Entflammbarkeit | HB | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes | |
Koeffizient der thermischen Ausdehnung | 1e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
5e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 5e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Schmelzpunkt | 220 °C Show Supplier Material materials with Schmelzpunkt of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Temperaturleitfähigkeit | 1.41e-07 mm²/s Show Supplier Material materials with Temperaturleitfähigkeit of 1.41e-07 mm²/s | dry | - | |||
Wärmeformbeständigkeitstemperatur | 210 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 210 °C | dry | ISO 75-1/-2 | 2 MPa | ||
220 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 220 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 4 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4 [-] | dry | IEC 60250 | 5GHz |
4.1 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4.1 [-] | dry | IEC 60250 | 1GHz | |
4.5 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4.5 [-] | dry | IEC 62631-2-1 | 1MHz | |
4.9 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4.9 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
5.5 [-] Show Supplier Material materials with Dielektrizitätskonstante of 5.5 [-] | dry | IEC 62631-2-1 | 100Hz | |
12 [-] Show Supplier Material materials with Dielektrizitätskonstante of 12 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Durchschlagfestigkeit | 25 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 25 kV/mm | conditioned | IEC 60243-1 | |
35 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 35 kV/mm | dry | IEC 60243-1 | ||
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | dry, conditioned | IEC 60112 | |
Surface resistivity | 1e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq | conditioned | IEC 62631-3-2 | |
Verlustfaktor | 116 [-] Show Supplier Material materials with Verlustfaktor of 116 [-] | dry | IEC 60250 | 5GHz |
127 [-] Show Supplier Material materials with Verlustfaktor of 127 [-] | dry | IEC 60250 | 1GHz | |
270 [-] Show Supplier Material materials with Verlustfaktor of 270 [-] | dry | IEC 62631-2-1 | 1MHz | |
360 [-] Show Supplier Material materials with Verlustfaktor of 360 [-] | dry | IEC 62631-2-1 | 100Hz | |
770 [-] Show Supplier Material materials with Verlustfaktor of 770 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
3250 [-] Show Supplier Material materials with Verlustfaktor of 3250 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density of melt | 1380.0 g/cm³ Show Supplier Material materials with Density of melt of 1380.0 g/cm³ | dry | - |
Specific heat capacity melt | 1900 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 1900 J/(kg·K) | dry | - |
Thermal conductivity of melt | 0.37 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.37 W/(m·K) | dry | - |
Technological properties
Property | ||
---|---|---|
Application areas | Timing drive systems | |
Certifications | Yellow Card Available | |
Fillers | 50% Glass Fiber |