Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.57 g/cm³ Show Supplier Material materials with Dichte of 1.57 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.7 % Show Supplier Material materials with Moisture absorption of 1.7 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 12 GPa Show Supplier Material materials with Biegemodul of 12 GPa | conditioned | ISO 178 | |
14.5 GPa Show Supplier Material materials with Biegemodul of 14.5 GPa | dry | ISO 178 | ||
Dehnung | 2.5 % Show Supplier Material materials with Dehnung of 2.5 % | dry | ISO 527-1/-2 | |
5 % Show Supplier Material materials with Dehnung of 5 % | conditioned | ISO 527-1/-2 | ||
Elastizitätsmodul | 12.5 GPa Show Supplier Material materials with Elastizitätsmodul of 12.5 GPa | conditioned | ISO 527-1/-2 | |
16.5 GPa Show Supplier Material materials with Elastizitätsmodul of 16.5 GPa | dry | ISO 527-1/-2 | ||
Flexural yield strength | 275 MPa Show Supplier Material materials with Flexural yield strength of 275 MPa | conditioned | ISO 178 | |
335 MPa Show Supplier Material materials with Flexural yield strength of 335 MPa | dry | ISO 178 | ||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 12 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 12 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 13 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 13 kJ/m² | dry | ISO 179/1eA | |
23 °C | 16 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 16 kJ/m² | conditioned | ISO 179/1eA | |
Zugfestigkeit | 165 MPa Show Supplier Material materials with Zugfestigkeit of 165 MPa | conditioned | ISO 527-1/-2 | |
220 MPa Show Supplier Material materials with Zugfestigkeit of 220 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Thickness | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|---|
Entflammbarkeit | HB | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes | |
Koeffizient der thermischen Ausdehnung | 1.5e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
6e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 6e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Schmelzpunkt | 220 °C Show Supplier Material materials with Schmelzpunkt of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Wärmeformbeständigkeitstemperatur | 200 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 200 °C | dry | ISO 75-1/-2 | 2 MPa | ||
215 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 215 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Elektrisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Durchschlagfestigkeit | 21 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 21 kV/mm | conditioned | IEC 60243-1 |
23 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 23 kV/mm | dry | IEC 60243-1 | |
Kriechstromfestigkeit | 450 V Show Supplier Material materials with Kriechstromfestigkeit of 450 V | dry | IEC 60112 |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | HVAC lamellae | |
Certifications | Yellow Card Available | |
Fillers | 50% Glass Fiber |