Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.11 g/cm³ Show Supplier Material materials with Dichte of 1.11 g/cm³ | dry | ISO 1183 |
Mechanisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-1/-2 | |
300 % Show Supplier Material materials with Dehnung of 300 % | dry | ISO 527-1/-2 | ||
Elastizitätsmodul | 0.04 GPa Show Supplier Material materials with Elastizitätsmodul of 0.04 GPa | dry | ISO 527-1/-2 | |
Härte, Shore D | 30 [-] Show Supplier Material materials with Härte, Shore D of 30 [-] | dry | ISO 868 | 3s |
Zugfestigkeit | 19 MPa Show Supplier Material materials with Zugfestigkeit of 19 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzpunkt | 195 °C Show Supplier Material materials with Schmelzpunkt of 195 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Schmelzvolumenflussrate | 230 °C | 34 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 34 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Certifications | Food Contact |