Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.41 g/cm³ Show Supplier Material materials with Dichte of 1.41 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.4 % Show Supplier Material materials with Moisture absorption of 0.4 % | dry | Sim. to ISO 62 |
Wasserabsorption | 3.5 % Show Supplier Material materials with Wasserabsorption of 3.5 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 235 % Show Supplier Material materials with Dehnung of 235 % | dry | ISO 527-1/-2 | ||
Elastizitätsmodul | 0.24 GPa Show Supplier Material materials with Elastizitätsmodul of 0.24 GPa | dry | ISO 527-1/-2 | ||
Härte, Shore D | 60 [-] Show Supplier Material materials with Härte, Shore D of 60 [-] | dry | ISO 868 | 3s | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 22 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 22 kJ/m² | dry | ISO 179/1eA | |
23 °C | 60 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 60 kJ/m² | dry | ISO 179/1eA | ||
Zugfestigkeit | 21.3 MPa Show Supplier Material materials with Zugfestigkeit of 21.3 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Thickness | Testing Standard | Comment |
---|---|---|---|---|---|
Entflammbarkeit | V-0 | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes |
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | 3 mm | IEC 60695-2-12 | |
Relative temperature index, electrical | 50 °C Show Supplier Material materials with Relative temperature index, electrical of 50 °C | dry | 2 mm | UL746B | |
Relative temperature index, mechanical impact | 50 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 50 °C | dry | 2 mm | UL746B | |
Relative temperature index, mechanical strength | 50 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 50 °C | dry | 2 mm | UL746B | |
Schmelzpunkt | 220 °C Show Supplier Material materials with Schmelzpunkt of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Elektrisch
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Schmelzvolumenflussrate | 230 °C | 18 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 18 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Optical Fiber Cable guides and connectors | |
Certifications | Yellow Card Available |