Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 0.95 g/cm³ Show Supplier Material materials with Dichte of 0.95 g/cm³ | dry | ISO 1183 |
Wasserabsorption | 0.8 % Show Supplier Material materials with Wasserabsorption of 0.8 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 650 % Show Supplier Material materials with Dehnung of 650 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 0.02 GPa Show Supplier Material materials with Elastizitätsmodul of 0.02 GPa | dry | ISO 527-1/-2 | |
Härte, Shore D | 25 [-] Show Supplier Material materials with Härte, Shore D of 25 [-] | dry | ISO 868 | 3s |
Zugfestigkeit | 9 MPa Show Supplier Material materials with Zugfestigkeit of 9 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Glasübergangstemperatur | -74 °C Show Supplier Material materials with Glasübergangstemperatur of -74 °C | dry | ASTM D5026/D7028 | DMTA (tan d) |
-45 °C Show Supplier Material materials with Glasübergangstemperatur of -45 °C | dry | ISO 11357-1/-2 | 10°C/min | |
Koeffizient der thermischen Ausdehnung | 2.2e-06 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.2e-06 1/K | dry | ISO 11359-1/-2 | Parallel |
2.2e-06 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.2e-06 1/K | dry | ISO 11359-1/-2 | Normal | |
Schmelzpunkt | 195 °C Show Supplier Material materials with Schmelzpunkt of 195 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Density of melt | 905 g/cm³ Show Supplier Material materials with Density of melt of 905 g/cm³ | dry | - | |
Schmelzvolumenflussrate | 190 °C | 5 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 5 cm³/10min | dry | ISO 1133 |
Technological properties
Property |
---|