Akulon® F130-C3

Want to keep this datasheet? Save it now in your required format

Description

Akulon® is our family of high performance polyamide 6 and polyamide 66 materials, used by customers across the world in applications ranging from automotive, electronics & electrical, to furniture and packaging.
We offer Akulon® grades for injection molding, blow molding and extrusion (including barrier film, stock shapes, convoluted tubes, and mono and multi filament).
In molded parts the material offers an excellent balance of easy design and processing with outstanding mechanical properties over a wide temperature range and in diverse conditions. Meanwhile for extrusion the strength, resilience and easy processing of Akulon® sets the market standards.

Datasheet URL:

Akulon® F130-C3

Diese Materialdaten wurden von DSM zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Eigenschaften

Allgemein

PropertyValueConditionTesting Standard

Coefficient of friction, kinetic

1 [-]

Show Supplier Material materials with Coefficient of friction, kinetic of 1 [-]

dry

ISO 8295

Coefficient of friction, static

1.2 [-]

Show Supplier Material materials with Coefficient of friction, static of 1.2 [-]

dry

ISO 8295

Dichte

1.13 g/cm³

Show Supplier Material materials with Dichte of 1.13 g/cm³

dry

ISO 1183

Moisture absorption

2.8 %

Show Supplier Material materials with Moisture absorption of 2.8 %

dry

Sim. to ISO 62

Wasserabsorption

9 %

Show Supplier Material materials with Wasserabsorption of 9 %

dry

Sim. to ISO 62

Mechanisch

PropertyValueConditionTesting StandardComment

Dehnung

350 %

Show Supplier Material materials with Dehnung of 350 %

dry

ISO 527-3

Parallel

Elastizitätsmodul

0.46 GPa

Show Supplier Material materials with Elastizitätsmodul of 0.46 GPa

dry

DSM-Method, 50 mm/min

Streckgrenze

31 MPa

Show Supplier Material materials with Streckgrenze of 31 MPa

dry

ISO 527-3

Parallel

Zugfestigkeit

82 MPa

Show Supplier Material materials with Zugfestigkeit of 82 MPa

dry

ISO 527-3

Parallel

Thermisch

PropertyValueConditionTesting StandardComment

Koeffizient der thermischen Ausdehnung

9e-07 1/K

Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 9e-07 1/K

dry

ISO 11359-1/-2

Parallel

Schmelzpunkt

220 °C

Show Supplier Material materials with Schmelzpunkt of 220 °C

dry

ISO 11357-1/-3

10°C/min

Spezifische Wärmekapazität

1550 J/(kg·K)

Show Supplier Material materials with Spezifische Wärmekapazität of 1550 J/(kg·K)

dry

-

2250 J/(kg·K)

Show Supplier Material materials with Spezifische Wärmekapazität of 2250 J/(kg·K)

dry

Optisch

PropertyValueConditionTesting Standard

Transparenz

83

dry

DSM method

Rheological Properties

PropertyTemperatureValueConditionTesting Standard

Melt viscosity

260 °C

810 Pa·s

Show Supplier Material materials with Melt viscosity of 810 Pa·s

dry

DSM method, 260 °C

Viscosity number

196 cm³/gr

Show Supplier Material materials with Viscosity number of 196 cm³/gr

dry

ISO 307, 1157, 1628

Technological properties