Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.57 g/cm³ Show Supplier Material materials with Dichte of 1.57 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.4 % Show Supplier Material materials with Moisture absorption of 1.4 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 16 GPa Show Supplier Material materials with Biegemodul of 16 GPa | dry | ISO 178 | |
Dehnung | 4.1 % Show Supplier Material materials with Dehnung of 4.1 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 15 GPa Show Supplier Material materials with Elastizitätsmodul of 15 GPa | dry | ISO 527-1/-2 | |
Flexural yield strength | 370 MPa Show Supplier Material materials with Flexural yield strength of 370 MPa | dry | ISO 178 | |
Schlagfestigkeit, Charpy gekerbt | 23 °C | 20 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 20 kJ/m² | dry | ISO 179/1eA |
Schlagzähigkeit, Charpy ungekerbt | 23 °C | 105 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 105 kJ/m² | dry | ISO 179/1eU |
Zugfestigkeit | 230 MPa Show Supplier Material materials with Zugfestigkeit of 230 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzpunkt | 220 °C Show Supplier Material materials with Schmelzpunkt of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Schmelzvolumenflussrate | 250 °C | 2 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 2 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Fillers | 50% Glass Fiber |