Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.25 g/cm³ Show Supplier Material materials with Dichte of 1.25 g/cm³ | dry | ISO 1183 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Dehnung | 1.3 % Show Supplier Material materials with Dehnung of 1.3 % | dry | ISO 527-1/-2 | |
150 °C | 3 % Show Supplier Material materials with Dehnung of 3 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 26 GPa Show Supplier Material materials with Elastizitätsmodul of 26 GPa | dry | ISO 527-1/-2 | |
150 °C | 11.8 GPa Show Supplier Material materials with Elastizitätsmodul of 11.8 GPa | dry | ISO 527-1/-2 | |
Schlagfestigkeit, Charpy gekerbt | 23 °C | 6 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 6 kJ/m² | dry | ISO 179/1eA |
Schlagzähigkeit, Charpy ungekerbt | 23 °C | 45 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 45 kJ/m² | dry | ISO 179/1eU |
Zugfestigkeit | 280 MPa Show Supplier Material materials with Zugfestigkeit of 280 MPa | dry | ISO 527-1/-2 | |
150 °C | 117 MPa Show Supplier Material materials with Zugfestigkeit of 117 MPa | dry | ISO 527-1/-2 |
Thermisch
Technological properties
Property | ||
---|---|---|
Fillers | 30% Carbon Fiber |