Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.26 g/cm³ Show Supplier Material materials with Dichte of 1.26 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.25 % Show Supplier Material materials with Moisture absorption of 0.25 % | dry | Sim. to ISO 62 |
Wasserabsorption | 0.6 % Show Supplier Material materials with Wasserabsorption of 0.6 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-1/-2 | ||
Elastizitätsmodul | 0.25 GPa Show Supplier Material materials with Elastizitätsmodul of 0.25 GPa | dry | ISO 527-1/-2 | ||
Elongation at yield | 23 % Show Supplier Material materials with Elongation at yield of 23 % | dry | ISO 527-1/-2 | ||
Härte, Shore D | 55.0 [-] Show Supplier Material materials with Härte, Shore D of 55.0 [-] | dry | ISO 868 | 15s | |
Reißfestigkeit | 165 kN/m Show Supplier Material materials with Reißfestigkeit of 165 kN/m | dry | ISO 34-1; Method B | ||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 6 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 6 kJ/m² | dry | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 6 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 6 kJ/m² | dry | ISO 179/1eU |
Thermisch
Property | Value | Condition | Thickness | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|---|
Entflammbarkeit | HB | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes | |
Koeffizient der thermischen Ausdehnung | 1.6e-06 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.6e-06 1/K | dry | ISO 11359-1/-2 | Parallel | ||
Relative temperature index, electrical | 160 °C Show Supplier Material materials with Relative temperature index, electrical of 160 °C | dry | 0.75 mm | UL746B | ||
Relative temperature index, mechanical impact | 120 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 120 °C | dry | 0.75 mm | UL746B | ||
Relative temperature index, mechanical strength | 150 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 150 °C | dry | 0.75 mm | UL746B | ||
Schmelzpunkt | 195 °C Show Supplier Material materials with Schmelzpunkt of 195 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Vicat-Erweichungstemperatur | 85 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 85 °C | dry | ISO 306 | 50°C/h 50N | ||
Wärmeformbeständigkeitstemperatur | 80 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 80 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Elektrisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | dry | IEC 60112 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Schmelzmassenflussrate | 230 °C | 9.5 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 9.5 g/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Convoluted Tubes | |
Certifications | Yellow Card Available |