Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.23 g/cm³ Show Supplier Material materials with Dichte of 1.23 g/cm³ | dry | ISO 1183 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Biegemodul | 0.31 GPa Show Supplier Material materials with Biegemodul of 0.31 GPa | dry | ISO 178 | ||
120 °C | 0.11 GPa Show Supplier Material materials with Biegemodul of 0.11 GPa | dry | ISO 178 | ||
Dehnung | 150 % Show Supplier Material materials with Dehnung of 150 % | dry | ISO 527-1/-2 | ||
610 % Show Supplier Material materials with Dehnung of 610 % | dry | ISO 527-1/-2 | |||
Elastizitätsmodul | 0.3 GPa Show Supplier Material materials with Elastizitätsmodul of 0.3 GPa | dry | ISO 527-1/-2 | ||
Härte, Shore D | 55.0 [-] Show Supplier Material materials with Härte, Shore D of 55.0 [-] | dry | ISO 868 | 3s | |
Reißfestigkeit | 131 kN/m Show Supplier Material materials with Reißfestigkeit of 131 kN/m | dry | ISO 34-1; Method B | ||
137 kN/m Show Supplier Material materials with Reißfestigkeit of 137 kN/m | dry | ISO 34-1; Method B | |||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 15 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 15 kJ/m² | dry | ISO 179/1eA | |
Zugfestigkeit | 30 MPa Show Supplier Material materials with Zugfestigkeit of 30 MPa | dry | ISO 527-1/-2 | ||
41 MPa Show Supplier Material materials with Zugfestigkeit of 41 MPa | dry | ISO 527-1/-2 | Normal |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Schmelzpunkt | 220 °C Show Supplier Material materials with Schmelzpunkt of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Vicat-Erweichungstemperatur | 105 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 105 °C | dry | ISO 306 | 50°C/h 50N | |
Wärmeformbeständigkeitstemperatur | 100 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 100 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Schmelzvolumenflussrate | 230 °C | 2.9 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 2.9 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Clean Air Inlet Ducts, Hot Charged Air Ducts, Cold Charged Air Ducts |