Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.25 g/cm³ Show Supplier Material materials with Dichte of 1.25 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2 % Show Supplier Material materials with Moisture absorption of 2 % | dry | Sim. to ISO 62 |
Wasserabsorption | 7.8 % Show Supplier Material materials with Wasserabsorption of 7.8 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 5.1 GPa Show Supplier Material materials with Biegemodul of 5.1 GPa | dry | ISO 178 | |
Dehnung | 3 % Show Supplier Material materials with Dehnung of 3 % | dry | ISO 527-1/-2 | |
6 % Show Supplier Material materials with Dehnung of 6 % | conditioned | ISO 527-1/-2 | ||
Elastizitätsmodul | 4 GPa Show Supplier Material materials with Elastizitätsmodul of 4 GPa | conditioned | ISO 527-1/-2 | |
6.5 GPa Show Supplier Material materials with Elastizitätsmodul of 6.5 GPa | dry | ISO 527-1/-2 | ||
Flexural yield strength | 175 MPa Show Supplier Material materials with Flexural yield strength of 175 MPa | dry | ISO 178 | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 3.5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 3.5 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 5 kJ/m² | dry | ISO 179/1eA | |
23 °C | 8 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 8 kJ/m² | conditioned | ISO 179/1eA | |
Zugfestigkeit | 80 MPa Show Supplier Material materials with Zugfestigkeit of 80 MPa | conditioned | ISO 527-1/-2 | |
115 MPa Show Supplier Material materials with Zugfestigkeit of 115 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Thickness | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|---|
Entflammbarkeit | HB | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes | |
Relative temperature index, electrical | 140 °C Show Supplier Material materials with Relative temperature index, electrical of 140 °C | dry | 0.71 mm | UL746B | ||
Relative temperature index, mechanical impact | 120 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 120 °C | dry | 0.71 mm | UL746B | ||
Relative temperature index, mechanical strength | 120 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 120 °C | dry | 0.71 mm | UL746B | ||
Schmelzpunkt | 260 °C Show Supplier Material materials with Schmelzpunkt of 260 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Wärmeformbeständigkeitstemperatur | 240 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 240 °C | dry | ISO 75-1/-2 | 2 MPa | ||
255 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 255 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available | |
Fillers | 15% Glass Fiber |