Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.14 g/cm³ Show Supplier Material materials with Dichte of 1.14 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.8 % Show Supplier Material materials with Moisture absorption of 2.8 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 2.6 GPa Show Supplier Material materials with Biegemodul of 2.6 GPa | dry | ISO 178 | |
Dehnung | 10.6 % Show Supplier Material materials with Dehnung of 10.6 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 2.7 GPa Show Supplier Material materials with Elastizitätsmodul of 2.7 GPa | dry | ISO 527-1/-2 | |
Elongation at yield | 4.4 % Show Supplier Material materials with Elongation at yield of 4.4 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 94 MPa Show Supplier Material materials with Flexural yield strength of 94 MPa | dry | ISO 178 | |
Schlagfestigkeit, Charpy gekerbt | 23 °C | 1.6 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 1.6 kJ/m² | dry | ISO 179/1eA |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Schmelzpunkt | 205 °C Show Supplier Material materials with Schmelzpunkt of 205 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Wärmeformbeständigkeitstemperatur | 60 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 60 °C | dry | ISO 75-1/-2 | 2 MPa | |
104 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 104 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Schmelzmassenflussrate | 230 °C | 11 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 11 g/10min | dry | ISO 1133 |
Schmelzvolumenflussrate | 230 °C | 9.6 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 9.6 cm³/10min | dry | ISO 1133 |
Viscosity number | 183 cm³/gr Show Supplier Material materials with Viscosity number of 183 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property |
---|