Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Bio-based content | 71 % Show Supplier Material materials with Bio-based content of 71 % | dry | ASTM D6866-12 Method B |
Dichte | 1.2 g/cm³ Show Supplier Material materials with Dichte of 1.2 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.7 % Show Supplier Material materials with Moisture absorption of 1.7 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 5 GPa Show Supplier Material materials with Biegemodul of 5 GPa | dry | ISO 178 | |
Dehnung | 3.5 % Show Supplier Material materials with Dehnung of 3.5 % | dry | ISO 527-1/-2 | |
6.5 % Show Supplier Material materials with Dehnung of 6.5 % | conditioned | ISO 527-1/-2 | ||
Elastizitätsmodul | 3.8 GPa Show Supplier Material materials with Elastizitätsmodul of 3.8 GPa | conditioned | ISO 527-1/-2 | |
5.6 GPa Show Supplier Material materials with Elastizitätsmodul of 5.6 GPa | dry | ISO 527-1/-2 | ||
Flexural yield strength | 160 MPa Show Supplier Material materials with Flexural yield strength of 160 MPa | dry | ISO 178 | |
Schlagfestigkeit, Charpy gekerbt | 23 °C | 5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 5 kJ/m² | dry | ISO 179/1eA |
Schlagzähigkeit, Charpy ungekerbt | 23 °C | 40 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 40 kJ/m² | dry | ISO 179/1eU |
Zugfestigkeit | 85 MPa Show Supplier Material materials with Zugfestigkeit of 85 MPa | conditioned | ISO 527-1/-2 | |
125 MPa Show Supplier Material materials with Zugfestigkeit of 125 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Schmelzpunkt | 250 °C Show Supplier Material materials with Schmelzpunkt of 250 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Wärmeformbeständigkeitstemperatur | 214 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 214 °C | dry | ISO 75-1/-2 | 2 MPa | |
242 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 242 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Technological properties
Property | ||
---|---|---|
Certifications | Food Contact | |
Fillers | 15% Glass Fiber |