Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.07 g/cm³ Show Supplier Material materials with Dichte of 1.07 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.3 % Show Supplier Material materials with Moisture absorption of 2.3 % | dry | Sim. to ISO 62 |
Wasserabsorption | 8.5 % Show Supplier Material materials with Wasserabsorption of 8.5 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 0.6 GPa Show Supplier Material materials with Biegemodul of 0.6 GPa | conditioned | ISO 178 | |
1.9 GPa Show Supplier Material materials with Biegemodul of 1.9 GPa | dry | ISO 178 | ||
Dehnung | -40 °C | 18 % Show Supplier Material materials with Dehnung of 18 % | dry | ISO 527-1/-2 |
50 % Show Supplier Material materials with Dehnung of 50 % | dry, conditioned | ISO 527-1/-2 | ||
Elastizitätsmodul | -40 °C | 2.3 GPa Show Supplier Material materials with Elastizitätsmodul of 2.3 GPa | dry | ISO 527-1/-2 |
0.62 GPa Show Supplier Material materials with Elastizitätsmodul of 0.62 GPa | conditioned | ISO 527-1/-2 | ||
2.1 GPa Show Supplier Material materials with Elastizitätsmodul of 2.1 GPa | dry | ISO 527-1/-2 | ||
100 °C | 0.27 GPa Show Supplier Material materials with Elastizitätsmodul of 0.27 GPa | dry | ISO 527-1/-2 | |
Elongation at yield | -40 °C | 8 % Show Supplier Material materials with Elongation at yield of 8 % | dry | ISO 527-1/-2 |
4 % Show Supplier Material materials with Elongation at yield of 4 % | dry | ISO 527-1/-2 | ||
30 % Show Supplier Material materials with Elongation at yield of 30 % | conditioned | ISO 527-1/-2 | ||
Flexural yield strength | 25 MPa Show Supplier Material materials with Flexural yield strength of 25 MPa | conditioned | ISO 178 | |
75 MPa Show Supplier Material materials with Flexural yield strength of 75 MPa | dry | ISO 178 | ||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 18 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 18 kJ/m² | dry | ISO 179/1eA |
-30 °C | 25 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 25 kJ/m² | conditioned | ISO 179/1eA | |
23 °C | 65 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 65 kJ/m² | dry | ISO 179/1eA | |
23 °C | 75 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 75 kJ/m² | conditioned | ISO 179/1eA | |
Streckgrenze | -40 °C | 80 MPa Show Supplier Material materials with Streckgrenze of 80 MPa | dry | ISO 527-1/-2 |
30 MPa Show Supplier Material materials with Streckgrenze of 30 MPa | conditioned | ISO 527-1/-2 | ||
52 MPa Show Supplier Material materials with Streckgrenze of 52 MPa | dry | ISO 527-1/-2 | ||
Zugfestigkeit | -40 °C | 60 MPa Show Supplier Material materials with Zugfestigkeit of 60 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 1.2e-06 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.2e-06 1/K | dry | ISO 11359-1/-2 | Parallel | |
1.2e-06 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.2e-06 1/K | dry | ISO 11359-1/-2 | Normal | ||
Temperaturleitfähigkeit | 9.37e-08 mm²/s Show Supplier Material materials with Temperaturleitfähigkeit of 9.37e-08 mm²/s | dry | - | ||
Wärmeformbeständigkeitstemperatur | 55 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 55 °C | dry | ISO 75-1/-2 | 2 MPa | |
130 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 130 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 2.7 [-] Show Supplier Material materials with Dielektrizitätskonstante of 2.7 [-] | dry | IEC 62631-2-1 | 1MHz |
3.1 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.1 [-] | dry | IEC 62631-2-1 | 100Hz | |
3.5 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.5 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
10 [-] Show Supplier Material materials with Dielektrizitätskonstante of 10 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Durchschlagfestigkeit | 20 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 20 kV/mm | conditioned | IEC 60243-1 | |
27 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 27 kV/mm | dry | IEC 60243-1 | ||
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | conditioned | IEC 60112 | |
Surface resistivity | 5e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 5e+14 Ω/sq | conditioned | IEC 62631-3-2 | |
Verlustfaktor | 30 [-] Show Supplier Material materials with Verlustfaktor of 30 [-] | dry | IEC 62631-2-1 | 100Hz |
160 [-] Show Supplier Material materials with Verlustfaktor of 160 [-] | dry | IEC 62631-2-1 | 1MHz | |
1000 [-] Show Supplier Material materials with Verlustfaktor of 1000 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
1600 [-] Show Supplier Material materials with Verlustfaktor of 1600 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Density of melt | 869 g/cm³ Show Supplier Material materials with Density of melt of 869 g/cm³ | dry | - | ||
Schmelzvolumenflussrate | 250 °C | 19 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 19 cm³/10min | dry | ISO 1133 | |
Schrumpfung | 1.4 % Show Supplier Material materials with Schrumpfung of 1.4 % | dry | ISO 294-4 | Parallel | |
1.7 % Show Supplier Material materials with Schrumpfung of 1.7 % | dry | ISO 294-4 | Normal | ||
Specific heat capacity melt | 2740 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 2740 J/(kg·K) | dry | - | ||
Thermal conductivity of melt | 0.22 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.22 W/(m·K) | dry | - |
Technological properties
Property | ||
---|---|---|
Application areas | Lawnmower Trimmer Heads, Lawnmower Trimmer Housings |