Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.55 g/cm³ Show Supplier Material materials with Dichte of 1.55 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.6 % Show Supplier Material materials with Moisture absorption of 1.6 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 7.2 GPa Show Supplier Material materials with Biegemodul of 7.2 GPa | conditioned | ISO 178 | |
12 GPa Show Supplier Material materials with Biegemodul of 12 GPa | dry | ISO 178 | ||
Dehnung | 2.5 % Show Supplier Material materials with Dehnung of 2.5 % | dry | ISO 527-1/-2 | |
5.2 % Show Supplier Material materials with Dehnung of 5.2 % | conditioned | ISO 527-1/-2 | ||
Elastizitätsmodul | 7.1 GPa Show Supplier Material materials with Elastizitätsmodul of 7.1 GPa | conditioned | ISO 527-1/-2 | |
12.5 GPa Show Supplier Material materials with Elastizitätsmodul of 12.5 GPa | dry | ISO 527-1/-2 | ||
Flexural yield strength | 135 MPa Show Supplier Material materials with Flexural yield strength of 135 MPa | conditioned | ISO 178 | |
200 MPa Show Supplier Material materials with Flexural yield strength of 200 MPa | dry | ISO 178 | ||
Schlagfestigkeit, Charpy gekerbt | 23 °C | 9 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 9 kJ/m² | dry | ISO 179/1eA |
23 °C | 13 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 13 kJ/m² | conditioned | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | 23 °C | 55.0 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 55.0 kJ/m² | dry | ISO 179/1eU |
23 °C | 60 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 60 kJ/m² | conditioned | ISO 179/1eU | |
Zugfestigkeit | 80 MPa Show Supplier Material materials with Zugfestigkeit of 80 MPa | conditioned | ISO 527-1/-2 | |
130 MPa Show Supplier Material materials with Zugfestigkeit of 130 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 2e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
9e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 9e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Wärmeformbeständigkeitstemperatur | 210 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 210 °C | dry | ISO 75-1/-2 | 2 MPa | |
Wärmeleitfähigkeit | 0.9 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 0.9 W/(m·K) | dry | ASTM E1461 | through plane | |
2.1 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 2.1 W/(m·K) | dry | ASTM E1461 | in plane |
Elektrisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Kriechstromfestigkeit | 350 V Show Supplier Material materials with Kriechstromfestigkeit of 350 V | dry | IEC 60112 |
Surface resistivity | 2e+11 Ω/sq Show Supplier Material materials with Surface resistivity of 2e+11 Ω/sq | conditioned | IEC 62631-3-2 |
Volume resistivity | 4e+12 Ω·cm Show Supplier Material materials with Volume resistivity of 4e+12 Ω·cm | conditioned | IEC 62631-3-1 |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Fillers | 20% Glass Fiber |