Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.39 g/cm³ Show Supplier Material materials with Dichte of 1.39 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.3 % Show Supplier Material materials with Moisture absorption of 0.3 % | dry | Sim. to ISO 62 |
Sauerstoffindex | 25 % Show Supplier Material materials with Sauerstoffindex of 25 % | dry | ISO 4589-1/-2 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 2.5 GPa Show Supplier Material materials with Elastizitätsmodul of 2.5 GPa | dry | ISO 527-1/-2 | |
Elongation at yield | 4 % Show Supplier Material materials with Elongation at yield of 4 % | dry | ISO 527-1/-2 | |
Schlagfestigkeit, Charpy gekerbt | 23 °C | 4 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 4 kJ/m² | dry | ISO 179/1eA |
Thermisch
Property | Value | Condition | Thickness | Testing Standard | Comment |
---|---|---|---|---|---|
Entflammbarkeit | HB | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes |
Relative temperature index, electrical | 75 °C Show Supplier Material materials with Relative temperature index, electrical of 75 °C | dry | 0.93 mm | UL746B | |
Relative temperature index, mechanical impact | 75 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 75 °C | dry | 0.93 mm | UL746B | |
Relative temperature index, mechanical strength | 75 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 75 °C | dry | 0.93 mm | UL746B | |
Schmelzpunkt | 255 °C Show Supplier Material materials with Schmelzpunkt of 255 °C | dry | ISO 11357-1/-3 | 10°C/min |
Elektrisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Schmelzvolumenflussrate | 270 °C | 6.5 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 6.5 cm³/10min | dry | ISO 1133 |
Technological properties
Property |
---|