Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Coefficient of friction, kinetic | 1 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 1 [-] | dry | ISO 8295 |
Coefficient of friction, static | 1.2 [-] Show Supplier Material materials with Coefficient of friction, static of 1.2 [-] | dry | ISO 8295 |
Dichte | 1.13 g/cm³ Show Supplier Material materials with Dichte of 1.13 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.5 % Show Supplier Material materials with Moisture absorption of 2.5 % | dry | Sim. to ISO 62 |
Wasserabsorption | 9.5 % Show Supplier Material materials with Wasserabsorption of 9.5 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-1/-2 | |
350 % Show Supplier Material materials with Dehnung of 350 % | dry | ISO 527-3 | Parallel | |
Elastizitätsmodul | 0.45 GPa Show Supplier Material materials with Elastizitätsmodul of 0.45 GPa | dry | DSM-Method, 50 mm/min | |
2.7 GPa Show Supplier Material materials with Elastizitätsmodul of 2.7 GPa | dry | ISO 527-1/-2 | ||
Elongation at yield | 4 % Show Supplier Material materials with Elongation at yield of 4 % | dry | ISO 527-1/-2 | |
Streckgrenze | 31 MPa Show Supplier Material materials with Streckgrenze of 31 MPa | dry | ISO 527-3 | Parallel |
78 MPa Show Supplier Material materials with Streckgrenze of 78 MPa | dry | ISO 527-1/-2 | ||
Zugfestigkeit | 83 MPa Show Supplier Material materials with Zugfestigkeit of 83 MPa | dry | ISO 527-3 | Parallel |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 9e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 9e-07 1/K | dry | ISO 11359-1/-2 | Parallel |
9e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 9e-07 1/K | dry | ISO 11359-1/-2 | Normal | |
Schmelzpunkt | 220 °C Show Supplier Material materials with Schmelzpunkt of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Spezifische Wärmekapazität | 1550 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 1550 J/(kg·K) | dry | - | |
2250 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 2250 J/(kg·K) | dry |
Optisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Transparenz | 83 | dry | DSM method |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Melt viscosity | 260 °C | 2250 Pa·s Show Supplier Material materials with Melt viscosity of 2250 Pa·s | dry | DSM method, 260 °C |
Viscosity number | 245 cm³/gr Show Supplier Material materials with Viscosity number of 245 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Application areas | Food Packaging Films, Cheese Packaging Blown Film, Meat Packaging Blown Film, Fish Packaging Blown Film, Medical Packaging Blown Film | |
Certifications | Food Contact |