Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.52 g/cm³ Show Supplier Material materials with Dichte of 1.52 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.15 % Show Supplier Material materials with Moisture absorption of 0.15 % | dry | Sim. to ISO 62 |
Wasserabsorption | 0.3 % Show Supplier Material materials with Wasserabsorption of 0.3 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Dehnung | 2.9 % Show Supplier Material materials with Dehnung of 2.9 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 10 GPa Show Supplier Material materials with Elastizitätsmodul of 10 GPa | dry | ISO 527-1/-2 | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 11 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 11 kJ/m² | dry | ISO 179/1eA |
23 °C | 9 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 9 kJ/m² | dry | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 60 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 60 kJ/m² | dry | ISO 179/1eU |
23 °C | 65 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 65 kJ/m² | dry | ISO 179/1eU | |
Zugfestigkeit | 140 MPa Show Supplier Material materials with Zugfestigkeit of 140 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 3.5e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 3.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
7e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 7e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Schmelzpunkt | 225 °C Show Supplier Material materials with Schmelzpunkt of 225 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Temperaturleitfähigkeit | 8.23e-08 mm²/s Show Supplier Material materials with Temperaturleitfähigkeit of 8.23e-08 mm²/s | dry | - | ||
Wärmeformbeständigkeitstemperatur | 205 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 205 °C | dry | ISO 75-1/-2 | 2 MPa | |
220 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 220 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 3.7 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.7 [-] | dry | IEC 62631-2-1 | 1MHz |
3.9 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.9 [-] | dry | IEC 62631-2-1 | 100Hz | |
Durchschlagfestigkeit | 30 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 30 kV/mm | dry | IEC 60243-1 | |
Kriechstromfestigkeit | 400 V Show Supplier Material materials with Kriechstromfestigkeit of 400 V | dry | IEC 60112 | |
Verlustfaktor | 25 [-] Show Supplier Material materials with Verlustfaktor of 25 [-] | dry | IEC 62631-2-1 | 100Hz |
170 [-] Show Supplier Material materials with Verlustfaktor of 170 [-] | dry | IEC 62631-2-1 | 1MHz | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Density of melt | 1220 g/cm³ Show Supplier Material materials with Density of melt of 1220 g/cm³ | dry | - | |
Schmelzvolumenflussrate | 250 °C | 11 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 11 cm³/10min | dry | ISO 1133 |
Specific heat capacity melt | 1850 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 1850 J/(kg·K) | dry | - | |
Thermal conductivity of melt | 0.185 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.185 W/(m·K) | dry | - |
Technological properties
Property | ||
---|---|---|
Fillers | 30% Glass Fiber |