Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.26 g/cm³ Show Supplier Material materials with Dichte of 1.26 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.18 % Show Supplier Material materials with Moisture absorption of 0.18 % | dry | Sim. to ISO 62 |
Wasserabsorption | 0.6 % Show Supplier Material materials with Wasserabsorption of 0.6 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-1/-2 | ||
300 % Show Supplier Material materials with Dehnung of 300 % | dry | ISO 527-1/-2 | |||
Elastizitätsmodul | 0.36 GPa Show Supplier Material materials with Elastizitätsmodul of 0.36 GPa | dry | ISO 527-1/-2 | ||
Härte, Shore D | 71 [-] Show Supplier Material materials with Härte, Shore D of 71 [-] | dry | ISO 868 | 3s | |
Schlagfestigkeit, Charpy gekerbt | 23 °C | 16 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 16 kJ/m² | dry | ISO 179/1eA | |
Zugfestigkeit | 30.8 MPa Show Supplier Material materials with Zugfestigkeit of 30.8 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 1.75e-06 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.75e-06 1/K | dry | ISO 11359-1/-2 | Parallel | |
1.75e-06 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.75e-06 1/K | dry | ISO 11359-1/-2 | Normal | ||
Schmelzpunkt | 216 °C Show Supplier Material materials with Schmelzpunkt of 216 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Wärmeformbeständigkeitstemperatur | 52 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 52 °C | dry | ISO 75-1/-2 | 2 MPa |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Schmelzmassenflussrate | 230 °C | 28.0 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 28.0 g/10min | dry | ISO 1133 | |
Schrumpfung | 1.75 % Show Supplier Material materials with Schrumpfung of 1.75 % | dry | Sim. to ISO 294-4 | Parallel | |
2 % Show Supplier Material materials with Schrumpfung of 2 % | dry | Sim. to ISO 294-4 | Normal |
Technological properties
Property |
---|