Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 0.83 g/cm³ Show Supplier Material materials with Dichte of 0.83 g/cm³ | dry | ISO 60 |
1.29 g/cm³ Show Supplier Material materials with Dichte of 1.29 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 0.15 % Show Supplier Material materials with Moisture absorption of 0.15 % | dry | Sim. to ISO 62 |
Wasserabsorption | 0.6 % Show Supplier Material materials with Wasserabsorption of 0.6 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-1/-2 | ||
250 % Show Supplier Material materials with Dehnung of 250 % | dry | ISO 527-1/-2 | |||
Elastizitätsmodul | 0.8 GPa Show Supplier Material materials with Elastizitätsmodul of 0.8 GPa | dry | ISO 527-1/-2 | ||
Elongation at yield | 17 % Show Supplier Material materials with Elongation at yield of 17 % | dry | ISO 527-1/-2 | ||
Härte, Shore D | 70 [-] Show Supplier Material materials with Härte, Shore D of 70 [-] | dry | ISO 868 | 3s | |
Reißfestigkeit | 215 kN/m Show Supplier Material materials with Reißfestigkeit of 215 kN/m | dry | ISO 34-1; Method B | ||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 6 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 6 kJ/m² | dry | ISO 179/1eA | |
23 °C | 10 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 10 kJ/m² | dry | ISO 179/1eA | ||
Zugfestigkeit | 43 MPa Show Supplier Material materials with Zugfestigkeit of 43 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Thickness | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|---|
Entflammbarkeit | HB | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes | |
Koeffizient der thermischen Ausdehnung | 1.65e-06 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.65e-06 1/K | dry | ISO 11359-1/-2 | Parallel | ||
1.65e-06 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.65e-06 1/K | dry | ISO 11359-1/-2 | Normal | |||
Relative temperature index, electrical | 50 °C Show Supplier Material materials with Relative temperature index, electrical of 50 °C | dry | 2 mm | UL746B | ||
Relative temperature index, mechanical impact | 50 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 50 °C | dry | 2 mm | UL746B | ||
Relative temperature index, mechanical strength | 50 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 50 °C | dry | 2 mm | UL746B | ||
Schmelzpunkt | 221 °C Show Supplier Material materials with Schmelzpunkt of 221 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Temperaturleitfähigkeit | 5.54e-08 mm²/s Show Supplier Material materials with Temperaturleitfähigkeit of 5.54e-08 mm²/s | dry | - | |||
Vicat-Erweichungstemperatur | 160 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 160 °C | dry | ISO 306 | 50°C/h 50N | ||
Wärmeformbeständigkeitstemperatur | 120 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 120 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 3.3 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.3 [-] | dry | IEC 62631-2-1 | 1MHz |
3.7 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.7 [-] | dry | IEC 62631-2-1 | 100Hz | |
Durchschlagfestigkeit | 23 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 23 kV/mm | dry | IEC 60243-1 | |
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | dry | IEC 60112 | |
Verlustfaktor | 300 [-] Show Supplier Material materials with Verlustfaktor of 300 [-] | dry | IEC 62631-2-1 | 1MHz |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Density of melt | 950 g/cm³ Show Supplier Material materials with Density of melt of 950 g/cm³ | dry | - | ||
Schmelzvolumenflussrate | 230 °C | 18 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 18 cm³/10min | dry | ISO 1133 | |
Schrumpfung | 1.75 % Show Supplier Material materials with Schrumpfung of 1.75 % | dry | Sim. to ISO 294-4 | Parallel | |
2 % Show Supplier Material materials with Schrumpfung of 2 % | dry | Sim. to ISO 294-4 | Normal | ||
Specific heat capacity melt | 1900 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 1900 J/(kg·K) | dry | - | ||
Thermal conductivity of melt | 0.1 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.1 W/(m·K) | dry | - |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available |