Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.36 g/cm³ Show Supplier Material materials with Dichte of 1.36 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.2 % Show Supplier Material materials with Moisture absorption of 2.2 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 5.5 GPa Show Supplier Material materials with Biegemodul of 5.5 GPa | conditioned | ISO 178 | |
8.5 GPa Show Supplier Material materials with Biegemodul of 8.5 GPa | dry | ISO 178 | ||
Dehnung | 3 % Show Supplier Material materials with Dehnung of 3 % | dry | ISO 527-1/-2 | |
7 % Show Supplier Material materials with Dehnung of 7 % | conditioned | ISO 527-1/-2 | ||
Elastizitätsmodul | 6.5 GPa Show Supplier Material materials with Elastizitätsmodul of 6.5 GPa | conditioned | ISO 527-1/-2 | |
9.6 GPa Show Supplier Material materials with Elastizitätsmodul of 9.6 GPa | dry | ISO 527-1/-2 | ||
Flexural yield strength | 175 MPa Show Supplier Material materials with Flexural yield strength of 175 MPa | conditioned | ISO 178 | |
270 MPa Show Supplier Material materials with Flexural yield strength of 270 MPa | dry | ISO 178 | ||
Schlagfestigkeit, Charpy gekerbt | 23 °C | 9.5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 9.5 kJ/m² | dry | ISO 179/1eA |
23 °C | 12 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 12 kJ/m² | conditioned | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | 23 °C | 65 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 65 kJ/m² | dry | ISO 179/1eU |
23 °C | 85 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 85 kJ/m² | conditioned | ISO 179/1eU | |
Zugfestigkeit | 115 MPa Show Supplier Material materials with Zugfestigkeit of 115 MPa | conditioned | ISO 527-1/-2 | |
170 MPa Show Supplier Material materials with Zugfestigkeit of 170 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 2e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
7e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 7e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Schmelzpunkt | 222 °C Show Supplier Material materials with Schmelzpunkt of 222 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Wärmeformbeständigkeitstemperatur | 196 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 196 °C | dry | ISO 75-1/-2 | 2 MPa | |
216 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 216 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | HVAC lamellae | |
Fillers | 30% Glass Fiber |