Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.22 g/cm³ Show Supplier Material materials with Dichte of 1.22 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.15 % Show Supplier Material materials with Moisture absorption of 0.15 % | dry | Sim. to ISO 62 |
Wasserabsorption | 0.4 % Show Supplier Material materials with Wasserabsorption of 0.4 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 2 GPa Show Supplier Material materials with Biegemodul of 2 GPa | dry | ISO 178 | |
Dehnung | 15 % Show Supplier Material materials with Dehnung of 15 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 2 GPa Show Supplier Material materials with Elastizitätsmodul of 2 GPa | dry | ISO 527-1/-2 | |
Elongation at yield | 3.2 % Show Supplier Material materials with Elongation at yield of 3.2 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 65 MPa Show Supplier Material materials with Flexural yield strength of 65 MPa | dry | ISO 178 | |
Schlagfestigkeit, Charpy gekerbt | 23 °C | 5.5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 5.5 kJ/m² | dry | ISO 179/1eA |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 9.5e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 9.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
9.5e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 9.5e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Wärmeformbeständigkeitstemperatur | 50 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 50 °C | dry | ISO 75-1/-2 | 2 MPa | |
125 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 125 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Technological properties
Property |
---|