Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.37 g/cm³ Show Supplier Material materials with Dichte of 1.37 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.2 % Show Supplier Material materials with Moisture absorption of 0.2 % | dry | Sim. to ISO 62 |
Wasserabsorption | 0.5 % Show Supplier Material materials with Wasserabsorption of 0.5 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Dehnung | 12 % Show Supplier Material materials with Dehnung of 12 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 2.8 GPa Show Supplier Material materials with Elastizitätsmodul of 2.8 GPa | dry | ISO 527-1/-2 | |
Elongation at yield | 4 % Show Supplier Material materials with Elongation at yield of 4 % | dry | ISO 527-1/-2 | |
Schlagfestigkeit, Charpy gekerbt | 23 °C | 3 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 3 kJ/m² | dry | ISO 179/1eA |
Thermisch
Property | Value | Condition | Thickness | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|---|
Entflammbarkeit | HB | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes | |
Koeffizient der thermischen Ausdehnung | 7e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 7e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
7e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 7e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Relative temperature index, electrical | 75 °C Show Supplier Material materials with Relative temperature index, electrical of 75 °C | dry | 0.75 mm | UL746B | ||
Relative temperature index, mechanical impact | 75 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 75 °C | dry | 0.75 mm | UL746B | ||
Relative temperature index, mechanical strength | 75 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 75 °C | dry | 0.75 mm | UL746B | ||
Schmelzpunkt | 255 °C Show Supplier Material materials with Schmelzpunkt of 255 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Wärmeformbeständigkeitstemperatur | 80 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 80 °C | dry | ISO 75-1/-2 | 2 MPa | ||
115 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 115 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 3.2 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.2 [-] | dry | IEC 62631-2-1 | 1MHz |
3.3 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.3 [-] | dry | IEC 62631-2-1 | 100Hz | |
Verlustfaktor | 20 [-] Show Supplier Material materials with Verlustfaktor of 20 [-] | dry | IEC 62631-2-1 | 100Hz |
21 [-] Show Supplier Material materials with Verlustfaktor of 21 [-] | dry | IEC 62631-2-1 | 1MHz | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available |