Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.51 g/cm³ Show Supplier Material materials with Dichte of 1.51 g/cm³ | dry | ISO 1183 |
Mechanisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Biegemodul | 13 GPa Show Supplier Material materials with Biegemodul of 13 GPa | dry | ISO 178 |
Dehnung | 2.7 % Show Supplier Material materials with Dehnung of 2.7 % | dry | ISO 527-1/-2 |
Elastizitätsmodul | 15 GPa Show Supplier Material materials with Elastizitätsmodul of 15 GPa | dry | ISO 527-1/-2 |
Flexural yield strength | 360 MPa Show Supplier Material materials with Flexural yield strength of 360 MPa | dry | ISO 178 |
Zugfestigkeit | 230 MPa Show Supplier Material materials with Zugfestigkeit of 230 MPa | dry | ISO 527-1/-2 |
Thermisch
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 3.5 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.5 [-] | dry | IEC 60250 | 1GHz |
3.5 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.5 [-] | dry | IEC 60250 | 5GHz | |
Verlustfaktor | 93 [-] Show Supplier Material materials with Verlustfaktor of 93 [-] | dry | IEC 60250 | 5GHz |
103 [-] Show Supplier Material materials with Verlustfaktor of 103 [-] | dry | IEC 60250 | 1GHz |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Spiral flow length | 100 | dry | - | 1.0 mm 1000 bar |
Technological properties
Property | ||
---|---|---|
Fillers | 50% Glass Fiber |