Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.13 g/cm³ Show Supplier Material materials with Dichte of 1.13 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.8 % Show Supplier Material materials with Moisture absorption of 2.8 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 500 % Show Supplier Material materials with Dehnung of 500 % | dry | ISO 527-3 | Parallel |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzpunkt | 193 °C Show Supplier Material materials with Schmelzpunkt of 193 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Schmelzmassenflussrate | 230 °C | 2.6 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 2.6 g/10min | dry | ISO 1133 |
Schmelzvolumenflussrate | 230 °C | 2.3 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 2.3 cm³/10min | dry | ISO 1133 |
Viscosity number | 246 cm³/gr Show Supplier Material materials with Viscosity number of 246 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Certifications | Food Contact |