Allgemein
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dichte | 1.25 g/cm³ Show Supplier Material materials with Dichte of 1.25 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 3.2 % Show Supplier Material materials with Moisture absorption of 3.2 % | dry | Sim. to ISO 62 | |
Wasserabsorption | 3.3 % Show Supplier Material materials with Wasserabsorption of 3.3 % | dry | ISO 62 | at 23°C after 24h |
11.4 % Show Supplier Material materials with Wasserabsorption of 11.4 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 0.9 GPa Show Supplier Material materials with Biegemodul of 0.9 GPa | conditioned | ISO 178 | |
2.6 GPa Show Supplier Material materials with Biegemodul of 2.6 GPa | dry | ISO 178 | ||
Dehnung | 30 % Show Supplier Material materials with Dehnung of 30 % | dry | ISO 527-1/-2 | |
50 % Show Supplier Material materials with Dehnung of 50 % | conditioned | ISO 527-1/-2 | ||
120 °C | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-1/-2 | |
160 °C | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-1/-2 | |
180 °C | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-1/-2 | |
200 °C | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | -40 °C | 3.4 GPa Show Supplier Material materials with Elastizitätsmodul of 3.4 GPa | dry | ISO 527-1/-2 |
1 GPa Show Supplier Material materials with Elastizitätsmodul of 1 GPa | conditioned | ISO 527-1/-2 | ||
2.9 GPa Show Supplier Material materials with Elastizitätsmodul of 2.9 GPa | dry | ISO 527-1/-2 | ||
120 °C | 0.75 GPa Show Supplier Material materials with Elastizitätsmodul of 0.75 GPa | dry | ISO 527-1/-2 | |
160 °C | 0.65 GPa Show Supplier Material materials with Elastizitätsmodul of 0.65 GPa | dry | ISO 527-1/-2 | |
180 °C | 0.6 GPa Show Supplier Material materials with Elastizitätsmodul of 0.6 GPa | dry | ISO 527-1/-2 | |
200 °C | 0.56 GPa Show Supplier Material materials with Elastizitätsmodul of 0.56 GPa | dry | ISO 527-1/-2 | |
Elongation at yield | -40 °C | 8 % Show Supplier Material materials with Elongation at yield of 8 % | dry | ISO 527-1/-2 |
20 % Show Supplier Material materials with Elongation at yield of 20 % | dry | ISO 527-1/-2 | ||
30 % Show Supplier Material materials with Elongation at yield of 30 % | conditioned | ISO 527-1/-2 | ||
Flexural yield strength | 115 MPa Show Supplier Material materials with Flexural yield strength of 115 MPa | dry | ISO 178 | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 5 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 7 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 7 kJ/m² | dry | ISO 179/1eA | |
23 °C | 15 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 15 kJ/m² | conditioned | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 150 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 150 kJ/m² | dry | ISO 179/1eU |
Streckgrenze | -40 °C | 120 MPa Show Supplier Material materials with Streckgrenze of 120 MPa | dry | ISO 527-1/-2 |
50 MPa Show Supplier Material materials with Streckgrenze of 50 MPa | conditioned | ISO 527-1/-2 | ||
90 MPa Show Supplier Material materials with Streckgrenze of 90 MPa | dry | ISO 527-1/-2 | ||
120 °C | 45 MPa Show Supplier Material materials with Streckgrenze of 45 MPa | dry | ISO 527-1/-2 | |
160 °C | 40 MPa Show Supplier Material materials with Streckgrenze of 40 MPa | dry | ISO 527-1/-2 | |
180 °C | 35 MPa Show Supplier Material materials with Streckgrenze of 35 MPa | dry | ISO 527-1/-2 | |
200 °C | 30 MPa Show Supplier Material materials with Streckgrenze of 30 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Thickness | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|---|
Entflammbarkeit | HB | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes | |
Glasübergangstemperatur | 75 °C Show Supplier Material materials with Glasübergangstemperatur of 75 °C | dry | ISO 11357-1/-2 | 10°C/min | ||
Koeffizient der thermischen Ausdehnung | 8.5e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 8.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
1.1e-06 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.1e-06 1/K | dry | ISO 11359-1/-2 | Normal | |||
Schmelzpunkt | 295 °C Show Supplier Material materials with Schmelzpunkt of 295 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Vicat-Erweichungstemperatur | 290 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 290 °C | dry | ISO 306 | 50°C/h 50N | ||
Wärmeformbeständigkeitstemperatur | 190 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 190 °C | dry | ISO 75-1/-2 | 2 MPa | ||
290 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 290 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Elektrisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Kriechstromfestigkeit | 400 V Show Supplier Material materials with Kriechstromfestigkeit of 400 V | dry | IEC 60112 |
Surface resistivity | 1e+13 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+13 Ω/sq | conditioned | IEC 62631-3-2 |
Volume resistivity | 1e+07 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+07 Ω·cm | conditioned | IEC 62631-3-1 |
1e+12 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+12 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schrumpfung | 2 % Show Supplier Material materials with Schrumpfung of 2 % | dry | Sim. to ISO 294-4 | Parallel |
2 % Show Supplier Material materials with Schrumpfung of 2 % | dry | Sim. to ISO 294-4 | Normal | |
Spiral flow length | 115 | dry | - | 1.0 mm 800 bar |
125 | dry | - | 1.0 mm 900 bar | |
135 | dry | - | 1.0 mm 1000 bar | |
Viscosity number | 180 cm³/gr Show Supplier Material materials with Viscosity number of 180 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Application areas | New Generation Slide Shoe Surfaces, MTF/DMF Components, Front End Accessory Drive Parts: Belt Tensioner,Damping bands, Shoes and Bushings, Shifter fork wear pad | |
Certifications | Yellow Card Available | |
Fillers | PTFE |