Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 0.82 g/cm³ Show Supplier Material materials with Dichte of 0.82 g/cm³ | dry | ISO 60 |
1.29 g/cm³ Show Supplier Material materials with Dichte of 1.29 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 0.15 % Show Supplier Material materials with Moisture absorption of 0.15 % | dry | Sim. to ISO 62 |
Wasserabsorption | 0.6 % Show Supplier Material materials with Wasserabsorption of 0.6 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Biegemodul | 1.1 GPa Show Supplier Material materials with Biegemodul of 1.1 GPa | dry | ISO 178 | ||
Dehnung | 250 % Show Supplier Material materials with Dehnung of 250 % | dry | ISO 527-1/-2 | ||
250 % Show Supplier Material materials with Dehnung of 250 % | dry | ISO 527-1/-2 | |||
570 % Show Supplier Material materials with Dehnung of 570 % | dry | ISO 527-1/-2 | |||
Elastizitätsmodul | 0.9 GPa Show Supplier Material materials with Elastizitätsmodul of 0.9 GPa | dry | ISO 527-1/-2 | ||
Elongation at yield | 20 % Show Supplier Material materials with Elongation at yield of 20 % | dry | ISO 527-1/-2 | ||
Härte, Shore D | 71 [-] Show Supplier Material materials with Härte, Shore D of 71 [-] | dry | ISO 868 | 3s | |
Reißfestigkeit | 231 kN/m Show Supplier Material materials with Reißfestigkeit of 231 kN/m | dry | ISO 34-1; Method B | ||
235 kN/m Show Supplier Material materials with Reißfestigkeit of 235 kN/m | dry | ISO 34-1; Method B | |||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 6 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 6 kJ/m² | dry | ISO 179/1eA | |
23 °C | 15 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 15 kJ/m² | dry | ISO 179/1eA | ||
Zugfestigkeit | 38 MPa Show Supplier Material materials with Zugfestigkeit of 38 MPa | dry | ISO 527-1/-2 | ||
58.0 MPa Show Supplier Material materials with Zugfestigkeit of 58.0 MPa | dry | ISO 527-1/-2 | Normal |
Thermisch
Property | Value | Condition | Thickness | Testing Standard | Comment |
---|---|---|---|---|---|
Entflammbarkeit | HB | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes |
Koeffizient der thermischen Ausdehnung | 1.65e-06 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.65e-06 1/K | dry | ISO 11359-1/-2 | Parallel | |
1.65e-06 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.65e-06 1/K | dry | ISO 11359-1/-2 | Normal | ||
Relative temperature index, electrical | 50 °C Show Supplier Material materials with Relative temperature index, electrical of 50 °C | dry | 2 mm | UL746B | |
Relative temperature index, mechanical impact | 50 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 50 °C | dry | 2 mm | UL746B | |
Relative temperature index, mechanical strength | 50 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 50 °C | dry | 2 mm | UL746B | |
Schmelzpunkt | 221 °C Show Supplier Material materials with Schmelzpunkt of 221 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Temperaturleitfähigkeit | 5.85e-08 mm²/s Show Supplier Material materials with Temperaturleitfähigkeit of 5.85e-08 mm²/s | dry | - | ||
Vicat-Erweichungstemperatur | 160 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 160 °C | dry | ISO 306 | 50°C/h 50N |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 3.4 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.4 [-] | dry | IEC 62631-2-1 | 1MHz |
3.7 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.7 [-] | dry | IEC 62631-2-1 | 100Hz | |
Durchschlagfestigkeit | 23 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 23 kV/mm | dry | IEC 60243-1 | |
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | dry | IEC 60112 | |
Verlustfaktor | 400 [-] Show Supplier Material materials with Verlustfaktor of 400 [-] | dry | IEC 62631-2-1 | 1MHz |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Density of melt | 900 g/cm³ Show Supplier Material materials with Density of melt of 900 g/cm³ | dry | - | |
Schmelzvolumenflussrate | 230 °C | 4 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 4 cm³/10min | dry | ISO 1133 |
Specific heat capacity melt | 1900 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 1900 J/(kg·K) | dry | - | |
Thermal conductivity of melt | 0.1 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.1 W/(m·K) | dry | - |
Technological properties
Property | ||
---|---|---|
Application areas | Snowboard Cover Laminates, Optical Fiber Cable Jackets | |
Certifications | Yellow Card Available |