Allgemein
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Bio-based content | 68 % Show Supplier Material materials with Bio-based content of 68 % | dry | ASTM D6866-12 Method B | |
Dichte | 1.16 g/cm³ Show Supplier Material materials with Dichte of 1.16 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 1.7 % Show Supplier Material materials with Moisture absorption of 1.7 % | dry | Sim. to ISO 62 | |
Sauerstoffindex | 36 % Show Supplier Material materials with Sauerstoffindex of 36 % | dry | ISO 4589-1/-2 | |
Wasserabsorption | 0.6 % Show Supplier Material materials with Wasserabsorption of 0.6 % | dry | ISO 62 | at 23°C after 24h |
4.8 % Show Supplier Material materials with Wasserabsorption of 4.8 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Thickness |
---|---|---|---|---|---|
Biegemodul | 2.3 GPa Show Supplier Material materials with Biegemodul of 2.3 GPa | conditioned | ISO 178 | ||
3.9 GPa Show Supplier Material materials with Biegemodul of 3.9 GPa | dry | ISO 178 | |||
Dehnung | 6 % Show Supplier Material materials with Dehnung of 6 % | dry | ISO 527-1/-2 | ||
30 % Show Supplier Material materials with Dehnung of 30 % | conditioned | ISO 527-1/-2 | |||
65 °C | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-1/-2 | ||
90 °C | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-1/-2 | ||
100 °C | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-1/-2 | ||
125 °C | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-1/-2 | ||
Elastizitätsmodul | 2.2 GPa Show Supplier Material materials with Elastizitätsmodul of 2.2 GPa | conditioned | ISO 527-1/-2 | ||
3.4 GPa Show Supplier Material materials with Elastizitätsmodul of 3.4 GPa | dry | ISO 527-1/-2 | 0.6 mm | ||
3.8 GPa Show Supplier Material materials with Elastizitätsmodul of 3.8 GPa | dry | ISO 527-1/-2 | |||
65 °C | 1.9 GPa Show Supplier Material materials with Elastizitätsmodul of 1.9 GPa | dry | ISO 527-1/-2 | ||
90 °C | 1.2 GPa Show Supplier Material materials with Elastizitätsmodul of 1.2 GPa | dry | ISO 527-1/-2 | ||
100 °C | 1.1 GPa Show Supplier Material materials with Elastizitätsmodul of 1.1 GPa | dry | ISO 527-1/-2 | ||
125 °C | 0.9 GPa Show Supplier Material materials with Elastizitätsmodul of 0.9 GPa | dry | ISO 527-1/-2 | ||
Elongation at yield | 4 % Show Supplier Material materials with Elongation at yield of 4 % | dry | ISO 527-1/-2 | ||
12.5 % Show Supplier Material materials with Elongation at yield of 12.5 % | conditioned | ISO 527-1/-2 | |||
Flexural yield strength | 65 MPa Show Supplier Material materials with Flexural yield strength of 65 MPa | conditioned | ISO 178 | ||
120 MPa Show Supplier Material materials with Flexural yield strength of 120 MPa | dry | ISO 178 | |||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 2.8 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 2.8 kJ/m² | dry | ISO 179/1eA | |
23 °C | 3 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 3 kJ/m² | dry | ISO 179/1eA | ||
23 °C | 5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 5 kJ/m² | conditioned | ISO 179/1eA | ||
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 85 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 85 kJ/m² | dry | ISO 179/1eU | |
23 °C | 75 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 75 kJ/m² | dry | ISO 179/1eU | ||
Streckgrenze | 50 MPa Show Supplier Material materials with Streckgrenze of 50 MPa | conditioned | ISO 527-1/-2 | ||
75 MPa Show Supplier Material materials with Streckgrenze of 75 MPa | dry | ISO 527-1/-2 | |||
65 °C | 47 MPa Show Supplier Material materials with Streckgrenze of 47 MPa | dry | ISO 527-1/-2 | ||
90 °C | 36 MPa Show Supplier Material materials with Streckgrenze of 36 MPa | dry | ISO 527-1/-2 | ||
100 °C | 33 MPa Show Supplier Material materials with Streckgrenze of 33 MPa | dry | ISO 527-1/-2 | ||
125 °C | 28.0 MPa Show Supplier Material materials with Streckgrenze of 28.0 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Thickness | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|---|
Entflammbarkeit | V-0 | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes | |
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | 0.75 mm | IEC 60695-2-12 | ||
Glow Wire Ignition Temperature | 960 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 960 °C | dry | 0.75 mm | IEC 60695-2-13 | ||
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | dry | 0.4 mm | UL746B | ||
Relative temperature index, mechanical impact | 95 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 95 °C | dry | 0.4 mm | UL746B | ||
Relative temperature index, mechanical strength | 115 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 115 °C | dry | 0.4 mm | UL746B | ||
Schmelzpunkt | 250 °C Show Supplier Material materials with Schmelzpunkt of 250 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Wärmeformbeständigkeitstemperatur | 110 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 110 °C | dry | ISO 75-1/-2 | 2 MPa | ||
190 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 190 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 3.45 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.45 [-] | dry | IEC 62631-2-1 | 1MHz |
3.85 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.85 [-] | dry | IEC 62631-2-1 | 100Hz | |
Durchschlagfestigkeit | 27 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 27 kV/mm | conditioned | IEC 60243-1 | |
32 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 32 kV/mm | dry | IEC 60243-1 | ||
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | dry, conditioned | IEC 60112 | |
Surface resistivity | 6e+13 Ω/sq Show Supplier Material materials with Surface resistivity of 6e+13 Ω/sq | conditioned | IEC 62631-3-2 | |
Verlustfaktor | 140 [-] Show Supplier Material materials with Verlustfaktor of 140 [-] | dry | IEC 62631-2-1 | 100Hz |
200 [-] Show Supplier Material materials with Verlustfaktor of 200 [-] | dry | IEC 62631-2-1 | 1MHz | |
Volume resistivity | 7e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 7e+11 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available |