Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.56 g/cm³ Show Supplier Material materials with Dichte of 1.56 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.6 % Show Supplier Material materials with Moisture absorption of 1.6 % | dry | Sim. to ISO 62 |
Wasserabsorption | 4.2 % Show Supplier Material materials with Wasserabsorption of 4.2 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Dehnung | 2.5 % Show Supplier Material materials with Dehnung of 2.5 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 16 GPa Show Supplier Material materials with Elastizitätsmodul of 16 GPa | dry | ISO 527-1/-2 | |
Schlagfestigkeit, Charpy gekerbt | 23 °C | 18 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 18 kJ/m² | dry | ISO 179/1eA |
Zugfestigkeit | 260 MPa Show Supplier Material materials with Zugfestigkeit of 260 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Thickness | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|---|
Relative temperature index, electrical | 85 °C Show Supplier Material materials with Relative temperature index, electrical of 85 °C | dry | 0.75 mm | UL746B | ||
Relative temperature index, mechanical impact | 85 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 85 °C | dry | 0.75 mm | UL746B | ||
Relative temperature index, mechanical strength | 85 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 85 °C | dry | 0.75 mm | UL746B | ||
Schmelzpunkt | 315 °C Show Supplier Material materials with Schmelzpunkt of 315 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Wärmeformbeständigkeitstemperatur | 245 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 245 °C | dry | ISO 75-1/-2 | 2 MPa |
Elektrisch
Rheological Properties
Technological properties
Property | ||
---|---|---|
Fillers | 50% Glass Fiber |