Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.73 g/cm³ Show Supplier Material materials with Dichte of 1.73 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.4 % Show Supplier Material materials with Moisture absorption of 1.4 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|---|
Biegemodul | 11 GPa Show Supplier Material materials with Biegemodul of 11 GPa | conditioned | ISO 178 | |||
14.5 GPa Show Supplier Material materials with Biegemodul of 14.5 GPa | dry | ISO 178 | ||||
120 °C | 9.5 GPa Show Supplier Material materials with Biegemodul of 9.5 GPa | dry | ISO 178 | |||
160 °C | 7.2 GPa Show Supplier Material materials with Biegemodul of 7.2 GPa | dry | ISO 178 | |||
Dehnung | 1.8 % Show Supplier Material materials with Dehnung of 1.8 % | dry | ISO 527-1/-2 | |||
1.9 % Show Supplier Material materials with Dehnung of 1.9 % | dry | ISO 527-1/-2 | 1 mm | |||
3 % Show Supplier Material materials with Dehnung of 3 % | conditioned | ISO 527-1/-2 | ||||
3 % Show Supplier Material materials with Dehnung of 3 % | conditioned | ISO 527-1/-2 | ||||
120 °C | 3.3 % Show Supplier Material materials with Dehnung of 3.3 % | dry | ISO 527-1/-2 | |||
160 °C | 4.5 % Show Supplier Material materials with Dehnung of 4.5 % | dry | ISO 527-1/-2 | |||
Elastizitätsmodul | 11 GPa Show Supplier Material materials with Elastizitätsmodul of 11 GPa | conditioned | ISO 527-1/-2 | |||
11.5 GPa Show Supplier Material materials with Elastizitätsmodul of 11.5 GPa | conditioned | ISO 527-1/-2 | ||||
16 GPa Show Supplier Material materials with Elastizitätsmodul of 16 GPa | dry | ISO 527-1/-2 | ||||
16 GPa Show Supplier Material materials with Elastizitätsmodul of 16 GPa | dry | ISO 527-1/-2 | 1 mm | |||
120 °C | 10 GPa Show Supplier Material materials with Elastizitätsmodul of 10 GPa | dry | ISO 527-1/-2 | |||
160 °C | 7.3 GPa Show Supplier Material materials with Elastizitätsmodul of 7.3 GPa | dry | ISO 527-1/-2 | |||
Flexural yield strength | 250 MPa Show Supplier Material materials with Flexural yield strength of 250 MPa | conditioned | ISO 178 | |||
310 MPa Show Supplier Material materials with Flexural yield strength of 310 MPa | dry | ISO 178 | ||||
120 °C | 200 MPa Show Supplier Material materials with Flexural yield strength of 200 MPa | dry | ISO 178 | |||
160 °C | 140 MPa Show Supplier Material materials with Flexural yield strength of 140 MPa | dry | ISO 178 | |||
Schlagfestigkeit, Charpy gekerbt | 23 °C | 14.0 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 14.0 kJ/m² | dry | ISO 179/1eA | ||
23 °C | 18 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 18 kJ/m² | conditioned | ISO 179/1eA | |||
Schlagzähigkeit, Charpy ungekerbt | 23 °C | 50 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 50 kJ/m² | dry | ISO 179/1eU | ||
23 °C | 70 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 70 kJ/m² | conditioned | ISO 179/1eU | |||
Zugfestigkeit | 160 MPa Show Supplier Material materials with Zugfestigkeit of 160 MPa | conditioned | ISO 527-1/-2 | |||
160 MPa Show Supplier Material materials with Zugfestigkeit of 160 MPa | conditioned | ISO 527-1/-2 | at low thickness | |||
210 MPa Show Supplier Material materials with Zugfestigkeit of 210 MPa | dry | ISO 527-1/-2 | ||||
220 MPa Show Supplier Material materials with Zugfestigkeit of 220 MPa | dry | ISO 527-1/-2 | 1 mm | at low thickness | ||
120 °C | 120 MPa Show Supplier Material materials with Zugfestigkeit of 120 MPa | dry | ISO 527-1/-2 | |||
160 °C | 100 MPa Show Supplier Material materials with Zugfestigkeit of 100 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Glasübergangstemperatur | 75 °C Show Supplier Material materials with Glasübergangstemperatur of 75 °C | dry | ISO 11357-1/-2 | 10°C/min | ||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | dry | UL746B | 3 mm | ||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | UL746B | 3 mm | ||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | dry | UL746B | 3 mm | ||
Schmelzpunkt | 295 °C Show Supplier Material materials with Schmelzpunkt of 295 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Wärmeformbeständigkeitstemperatur | 280 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 280 °C | dry | ISO 75-1/-2 | 2 MPa |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | DDR DIMM Connectors, Reflow connectors (2) | |
Certifications | Yellow Card Available | |
Fillers | 43% Glass Fiber |