Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.12 g/cm³ Show Supplier Material materials with Dichte of 1.12 g/cm³ | dry | ISO 1183 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 0.98 GPa Show Supplier Material materials with Biegemodul of 0.98 GPa | conditioned | ISO 178 | |
2.4 GPa Show Supplier Material materials with Biegemodul of 2.4 GPa | dry | ISO 178 | ||
Dehnung | 12 % Show Supplier Material materials with Dehnung of 12 % | dry | ISO 527-1/-2 | |
13 % Show Supplier Material materials with Dehnung of 13 % | dry | ISO 527-1/-2 | ||
50 % Show Supplier Material materials with Dehnung of 50 % | conditioned | ISO 527-1/-2 | ||
Elastizitätsmodul | 2.5 GPa Show Supplier Material materials with Elastizitätsmodul of 2.5 GPa | dry | ISO 527-1/-2 | |
Elongation at yield | 4.3 % Show Supplier Material materials with Elongation at yield of 4.3 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 48 MPa Show Supplier Material materials with Flexural yield strength of 48 MPa | conditioned | ISO 178 | |
95 MPa Show Supplier Material materials with Flexural yield strength of 95 MPa | dry | ISO 178 | ||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 5 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 8 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 8 kJ/m² | dry | ISO 179/1eA | |
23 °C | 20 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 20 kJ/m² | conditioned | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 280 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 280 kJ/m² | dry, conditioned | ISO 179/1eU |
Zugfestigkeit | 50 MPa Show Supplier Material materials with Zugfestigkeit of 50 MPa | dry | ISO 527-1/-2 |