Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dichte | 1.27 g/cm³ Show Supplier Material materials with Dichte of 1.27 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 0.1 % Show Supplier Material materials with Moisture absorption of 0.1 % | dry | Sim. to ISO 62 | |
Wasserabsorption | 0.22 % Show Supplier Material materials with Wasserabsorption of 0.22 % | dry | ISO 62 | at 23°C after 24h |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Biegemodul | 0.27 GPa Show Supplier Material materials with Biegemodul of 0.27 GPa | dry | ISO 178 | ||
Dehnung | 300 % Show Supplier Material materials with Dehnung of 300 % | dry | ISO 527-1/-2 | ||
520 % Show Supplier Material materials with Dehnung of 520 % | dry | ISO 527-1/-2 | |||
640 % Show Supplier Material materials with Dehnung of 640 % | dry | ISO 527-1/-2 | |||
Elastizitätsmodul | 0.31 GPa Show Supplier Material materials with Elastizitätsmodul of 0.31 GPa | dry | ISO 527-1/-2 | ||
Härte, Shore A | 98 [-] Show Supplier Material materials with Härte, Shore A of 98 [-] | dry | ISO 868 | 3s | |
98 [-] Show Supplier Material materials with Härte, Shore A of 98 [-] | dry | ISO 868 | 15s | ||
Härte, Shore D | 61 [-] Show Supplier Material materials with Härte, Shore D of 61 [-] | dry | ISO 868 | 3s | |
61 [-] Show Supplier Material materials with Härte, Shore D of 61 [-] | dry | ISO 868 | 15s | ||
Reißfestigkeit | 171 kN/m Show Supplier Material materials with Reißfestigkeit of 171 kN/m | dry | ISO 34-1; Method B | ||
191 kN/m Show Supplier Material materials with Reißfestigkeit of 191 kN/m | dry | ISO 34-1; Method B | |||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 5 kJ/m² | dry | ISO 179/1eA | |
Zugfestigkeit | 33 MPa Show Supplier Material materials with Zugfestigkeit of 33 MPa | dry | ISO 527-1/-2 | ||
40 MPa Show Supplier Material materials with Zugfestigkeit of 40 MPa | dry | ISO 527-1/-2 | Normal |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Glasübergangstemperatur | -10 °C Show Supplier Material materials with Glasübergangstemperatur of -10 °C | dry | ISO 11357-1/-2 | 10°C/min |
Schmelzpunkt | 208 °C Show Supplier Material materials with Schmelzpunkt of 208 °C | dry | ISO 11357-1/-3 | 10°C/min |
Vicat-Erweichungstemperatur | 90 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 90 °C | dry | ISO 306 | 50°C/h 50N |
190 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 190 °C | dry | ISO 306 | 50°C/h 10N |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Schmelzvolumenflussrate | 230 °C | 9 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 9 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Brake Tubing with Arnitel® CM622, Wire and Cable Insulation, Convoluted Tubes |