Allgemein
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dichte | 1.65 g/cm³ Show Supplier Material materials with Dichte of 1.65 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 0.04 % Show Supplier Material materials with Moisture absorption of 0.04 % | dry | Sim. to ISO 62 | |
Wasserabsorption | 0.04 % Show Supplier Material materials with Wasserabsorption of 0.04 % | dry | ISO 62 | at 23°C after 24h |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 14.5 GPa Show Supplier Material materials with Biegemodul of 14.5 GPa | dry | ISO 178 | |
120 °C | 10 GPa Show Supplier Material materials with Biegemodul of 10 GPa | dry | ISO 178 | |
160 °C | 5 GPa Show Supplier Material materials with Biegemodul of 5 GPa | dry | ISO 178 | |
200 °C | 4.2 GPa Show Supplier Material materials with Biegemodul of 4.2 GPa | dry | ISO 178 | |
Dehnung | -40 °C | 2 % Show Supplier Material materials with Dehnung of 2 % | dry | ISO 527-1/-2 |
2 % Show Supplier Material materials with Dehnung of 2 % | dry | ISO 527-1/-2 | ||
120 °C | 3.1 % Show Supplier Material materials with Dehnung of 3.1 % | dry | ISO 527-1/-2 | |
160 °C | 3.9 % Show Supplier Material materials with Dehnung of 3.9 % | dry | ISO 527-1/-2 | |
200 °C | 6.4 % Show Supplier Material materials with Dehnung of 6.4 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | -40 °C | 16 GPa Show Supplier Material materials with Elastizitätsmodul of 16 GPa | dry | ISO 527-1/-2 |
15 GPa Show Supplier Material materials with Elastizitätsmodul of 15 GPa | dry | ISO 527-1/-2 | ||
120 °C | 7.3 GPa Show Supplier Material materials with Elastizitätsmodul of 7.3 GPa | dry | ISO 527-1/-2 | |
160 °C | 5.2 GPa Show Supplier Material materials with Elastizitätsmodul of 5.2 GPa | dry | ISO 527-1/-2 | |
200 °C | 3.4 GPa Show Supplier Material materials with Elastizitätsmodul of 3.4 GPa | dry | ISO 527-1/-2 | |
Flexural yield strength | 300 MPa Show Supplier Material materials with Flexural yield strength of 300 MPa | dry | ISO 178 | |
120 °C | 150 MPa Show Supplier Material materials with Flexural yield strength of 150 MPa | dry | ISO 178 | |
160 °C | 100 MPa Show Supplier Material materials with Flexural yield strength of 100 MPa | dry | ISO 178 | |
200 °C | 80 MPa Show Supplier Material materials with Flexural yield strength of 80 MPa | dry | ISO 178 | |
Hardness, Rockwell R | 121 [-] Show Supplier Material materials with Hardness, Rockwell R of 121 [-] | dry | ISO 2039-2 | |
Härte, Rockwell M | 100 [-] Show Supplier Material materials with Härte, Rockwell M of 100 [-] | dry | ISO 2039-2 | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 11 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 11 kJ/m² | dry | ISO 179/1eA |
23 °C | 11 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 11 kJ/m² | dry | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 57.0 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 57.0 kJ/m² | dry | ISO 179/1eU |
23 °C | 48 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 48 kJ/m² | dry | ISO 180/1U | |
23 °C | 56.0 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 56.0 kJ/m² | dry | ISO 179/1eU | |
Zugfestigkeit | -40 °C | 235 MPa Show Supplier Material materials with Zugfestigkeit of 235 MPa | dry | ISO 527-1/-2 |
200 MPa Show Supplier Material materials with Zugfestigkeit of 200 MPa | dry | ISO 527-1/-2 | ||
120 °C | 105 MPa Show Supplier Material materials with Zugfestigkeit of 105 MPa | dry | ISO 527-1/-2 | |
160 °C | 73 MPa Show Supplier Material materials with Zugfestigkeit of 73 MPa | dry | ISO 527-1/-2 | |
200 °C | 55.0 MPa Show Supplier Material materials with Zugfestigkeit of 55.0 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Thickness | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|---|
Entflammbarkeit | V-0 | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes | |
Glasübergangstemperatur | 90 °C Show Supplier Material materials with Glasübergangstemperatur of 90 °C | dry | ISO 11357-1/-2 | 10°C/min | ||
Koeffizient der thermischen Ausdehnung | 1.3e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.3e-07 1/K | dry | ISO 11359-1/-2 | parallel, above Tg | ||
1.6e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.6e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |||
4e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 4e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
8.5e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 8.5e-07 1/K | dry | ISO 11359-1/-2 | normal, above Tg | |||
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | dry | 0.8 mm | UL746B | ||
Relative temperature index, mechanical impact | 130 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 130 °C | dry | 0.8 mm | UL746B | ||
Relative temperature index, mechanical strength | 130 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C | dry | 0.8 mm | UL746B | ||
Schmelzpunkt | 280 °C Show Supplier Material materials with Schmelzpunkt of 280 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Wärmeformbeständigkeitstemperatur | 185 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 185 °C | dry | ISO 75-1/-2 | 8 MPa | ||
265 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 265 °C | dry | ISO 75-1/-2 | 2 MPa | |||
280 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 280 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 4 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4 [-] | dry | IEC 60250 | 1GHz |
4 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4 [-] | dry | IEC 60250 | 5GHz | |
Durchschlagfestigkeit | 31 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 31 kV/mm | dry | IEC 60234 | |
32 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 32 kV/mm | dry | IEC 60243-1 | ||
Kriechstromfestigkeit | 175 V Show Supplier Material materials with Kriechstromfestigkeit of 175 V | dry | IEC 60112 | |
Surface resistivity | 1e+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+15 Ω/sq | dry | IEC 62631-3-2 | |
Verlustfaktor | 35 [-] Show Supplier Material materials with Verlustfaktor of 35 [-] | dry | IEC 60250 | 1GHz |
55 [-] Show Supplier Material materials with Verlustfaktor of 55 [-] | dry | IEC 60250 | 5GHz | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Coil insulation, Automotive e-motor Bobbins, Internal structure for mini projector | |
Fillers | 40% Glass Fiber |