Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.33 g/cm³ Show Supplier Material materials with Dichte of 1.33 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.18 % Show Supplier Material materials with Moisture absorption of 0.18 % | dry | Sim. to ISO 62 |
Wasserabsorption | 0.45 % Show Supplier Material materials with Wasserabsorption of 0.45 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Dehnung | 20 % Show Supplier Material materials with Dehnung of 20 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 2.7 GPa Show Supplier Material materials with Elastizitätsmodul of 2.7 GPa | dry | ISO 527-1/-2 | |
Elongation at yield | 3.5 % Show Supplier Material materials with Elongation at yield of 3.5 % | dry | ISO 527-1/-2 | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 5 kJ/m² | dry | ISO 179/1eA |
23 °C | 5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 5 kJ/m² | dry | ISO 179/1eA |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 9e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 9e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
9e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 9e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Schmelzpunkt | 225 °C Show Supplier Material materials with Schmelzpunkt of 225 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Temperaturleitfähigkeit | 4.65e-08 mm²/s Show Supplier Material materials with Temperaturleitfähigkeit of 4.65e-08 mm²/s | dry | - | ||
Wärmeformbeständigkeitstemperatur | 55 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 55 °C | dry | ISO 75-1/-2 | 2 MPa | |
165 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 165 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 3.2 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.2 [-] | dry | IEC 62631-2-1 | 1MHz |
3.5 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.5 [-] | dry | IEC 62631-2-1 | 100Hz | |
Durchschlagfestigkeit | 27 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 27 kV/mm | dry | IEC 60243-1 | |
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | dry | IEC 60112 | |
Verlustfaktor | 20 [-] Show Supplier Material materials with Verlustfaktor of 20 [-] | dry | IEC 62631-2-1 | 100Hz |
200 [-] Show Supplier Material materials with Verlustfaktor of 200 [-] | dry | IEC 62631-2-1 | 1MHz | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Density of melt | 1040 g/cm³ Show Supplier Material materials with Density of melt of 1040 g/cm³ | dry | - | ||
Schmelzmassenflussrate | 27 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 27 g/10min | dry | ISO 1133 | ||
Schmelzvolumenflussrate | 250 °C | 24 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 24 cm³/10min | dry | ISO 1133 | |
Schrumpfung | 2 % Show Supplier Material materials with Schrumpfung of 2 % | dry | Sim. to ISO 294-4 | Parallel | |
2 % Show Supplier Material materials with Schrumpfung of 2 % | dry | Sim. to ISO 294-4 | Normal | ||
Specific heat capacity melt | 2260 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 2260 J/(kg·K) | dry | - | ||
Thermal conductivity of melt | 0.109 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.109 W/(m·K) | dry | - |
Technological properties
Property | ||
---|---|---|
Application areas | Inhaler components |