Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 0.69 g/cm³ Show Supplier Material materials with Dichte of 0.69 g/cm³ | dry | ISO 60 |
1.11 g/cm³ Show Supplier Material materials with Dichte of 1.11 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 0.3 % Show Supplier Material materials with Moisture absorption of 0.3 % | dry | Sim. to ISO 62 |
Wasserabsorption | 0.75 % Show Supplier Material materials with Wasserabsorption of 0.75 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-1/-2 | |
300 % Show Supplier Material materials with Dehnung of 300 % | dry | ISO 527-1/-2 | ||
Elastizitätsmodul | 0.04 GPa Show Supplier Material materials with Elastizitätsmodul of 0.04 GPa | dry | ISO 527-1/-2 | |
Elongation at yield | 77 % Show Supplier Material materials with Elongation at yield of 77 % | dry | ISO 527-1/-2 | |
Härte, Shore D | 33 [-] Show Supplier Material materials with Härte, Shore D of 33 [-] | dry | ISO 868 | 3s |
Zugfestigkeit | 21 MPa Show Supplier Material materials with Zugfestigkeit of 21 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Thickness | Testing Standard | Comment |
---|---|---|---|---|---|
Entflammbarkeit | HB | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes |
Glasübergangstemperatur | -78 °C Show Supplier Material materials with Glasübergangstemperatur of -78 °C | dry | ISO 11357-1/-2 | 10°C/min | |
Koeffizient der thermischen Ausdehnung | 2.2e-06 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.2e-06 1/K | dry | ISO 11359-1/-2 | Parallel | |
2.2e-06 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.2e-06 1/K | dry | ISO 11359-1/-2 | Normal | ||
Relative temperature index, electrical | 50 °C Show Supplier Material materials with Relative temperature index, electrical of 50 °C | dry | 2 mm | UL746B | |
Relative temperature index, mechanical impact | 50 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 50 °C | dry | 2 mm | UL746B | |
Relative temperature index, mechanical strength | 50 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 50 °C | dry | 2 mm | UL746B | |
Schmelzpunkt | 195 °C Show Supplier Material materials with Schmelzpunkt of 195 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Temperaturleitfähigkeit | 6.56e-08 mm²/s Show Supplier Material materials with Temperaturleitfähigkeit of 6.56e-08 mm²/s | dry | - |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 4 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4 [-] | dry | IEC 62631-2-1 | 1MHz |
4.1 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4.1 [-] | dry | IEC 62631-2-1 | 100Hz | |
Durchschlagfestigkeit | 20 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 20 kV/mm | dry | IEC 60243-1 | |
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | dry | IEC 60112 | |
Verlustfaktor | 10 [-] Show Supplier Material materials with Verlustfaktor of 10 [-] | dry | IEC 62631-2-1 | 100Hz |
170 [-] Show Supplier Material materials with Verlustfaktor of 170 [-] | dry | IEC 62631-2-1 | 1MHz | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Density of melt | 896 g/cm³ Show Supplier Material materials with Density of melt of 896 g/cm³ | dry | - | ||
Schmelzvolumenflussrate | 230 °C | 33 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 33 cm³/10min | dry | ISO 1133 | |
Schrumpfung | 1.5 % Show Supplier Material materials with Schrumpfung of 1.5 % | dry | Sim. to ISO 294-4 | Parallel | |
1.5 % Show Supplier Material materials with Schrumpfung of 1.5 % | dry | Sim. to ISO 294-4 | Normal | ||
Specific heat capacity melt | 1700.0 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 1700.0 J/(kg·K) | dry | - | ||
Thermal conductivity of melt | 0.1 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.1 W/(m·K) | dry | - |
Technological properties
Property | ||
---|---|---|