Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.2 g/cm³ Show Supplier Material materials with Dichte of 1.2 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2 % Show Supplier Material materials with Moisture absorption of 2 % | dry | Sim. to ISO 62 |
Wasserabsorption | 6.8 % Show Supplier Material materials with Wasserabsorption of 6.8 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 5 GPa Show Supplier Material materials with Biegemodul of 5 GPa | dry | ISO 178 | |
Dehnung | 5 % Show Supplier Material materials with Dehnung of 5 % | dry | ISO 527-1/-2 | |
15 % Show Supplier Material materials with Dehnung of 15 % | conditioned | ISO 527-1/-2 | ||
Elastizitätsmodul | 3 GPa Show Supplier Material materials with Elastizitätsmodul of 3 GPa | conditioned | ISO 527-1/-2 | |
5.6 GPa Show Supplier Material materials with Elastizitätsmodul of 5.6 GPa | dry | ISO 527-1/-2 | ||
Flexural yield strength | 180 MPa Show Supplier Material materials with Flexural yield strength of 180 MPa | dry | ISO 178 | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 10 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 10 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 20 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 20 kJ/m² | dry | ISO 179/1eA | |
23 °C | 30 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 30 kJ/m² | conditioned | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 90 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 90 kJ/m² | dry, conditioned | ISO 179/1eU |
23 °C | 80 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 80 kJ/m² | dry | ISO 179/1eU | |
Zugfestigkeit | 60 MPa Show Supplier Material materials with Zugfestigkeit of 60 MPa | conditioned | ISO 527-1/-2 | |
110 MPa Show Supplier Material materials with Zugfestigkeit of 110 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Schmelzpunkt | 220 °C Show Supplier Material materials with Schmelzpunkt of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Wärmeformbeständigkeitstemperatur | 185 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 185 °C | dry | ISO 75-1/-2 | 2 MPa | |
210 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 210 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Schmelzvolumenflussrate | 275 °C | 40 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 40 cm³/10min | dry | ISO 1133 | |
Schrumpfung | 0.25 % Show Supplier Material materials with Schrumpfung of 0.25 % | dry | ISO 294-4 | Parallel | |
1.2 % Show Supplier Material materials with Schrumpfung of 1.2 % | dry | ISO 294-4 | Normal |
Technological properties
Property | ||
---|---|---|
Fillers | 15% Glass Fiber |