Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.21 g/cm³ Show Supplier Material materials with Dichte of 1.21 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.3 % Show Supplier Material materials with Moisture absorption of 2.3 % | dry | Sim. to ISO 62 |
Wasserabsorption | 7.7 % Show Supplier Material materials with Wasserabsorption of 7.7 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 4.2 GPa Show Supplier Material materials with Biegemodul of 4.2 GPa | dry | ISO 178 | |
Dehnung | 4 % Show Supplier Material materials with Dehnung of 4 % | dry | ISO 527-1/-2 | |
9 % Show Supplier Material materials with Dehnung of 9 % | conditioned | ISO 527-1/-2 | ||
Elastizitätsmodul | 2.9 GPa Show Supplier Material materials with Elastizitätsmodul of 2.9 GPa | conditioned | ISO 527-1/-2 | |
4.5 GPa Show Supplier Material materials with Elastizitätsmodul of 4.5 GPa | dry | ISO 527-1/-2 | ||
Flexural yield strength | 150 MPa Show Supplier Material materials with Flexural yield strength of 150 MPa | dry | ISO 178 | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 3 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 3 kJ/m² | dry | ISO 179/1eA |
-30 °C | 3.1 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 3.1 kJ/m² | conditioned | ISO 179/1eA | |
23 °C | 3.8 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 3.8 kJ/m² | dry | ISO 179/1eA | |
23 °C | 7 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 7 kJ/m² | conditioned | ISO 179/1eA | |
Zugfestigkeit | 68 MPa Show Supplier Material materials with Zugfestigkeit of 68 MPa | conditioned | ISO 527-1/-2 | |
100 MPa Show Supplier Material materials with Zugfestigkeit of 100 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Thickness | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|---|
Entflammbarkeit | HB | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes | |
Koeffizient der thermischen Ausdehnung | 3.5e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 3.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
1.2e-06 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.2e-06 1/K | dry | ISO 11359-1/-2 | Normal | |||
Relative temperature index, electrical | 140 °C Show Supplier Material materials with Relative temperature index, electrical of 140 °C | dry | 0.71 mm | UL746B | ||
Relative temperature index, mechanical impact | 120 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 120 °C | dry | 0.71 mm | UL746B | ||
Relative temperature index, mechanical strength | 140 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 140 °C | dry | 0.71 mm | UL746B | ||
Schmelzpunkt | 220 °C Show Supplier Material materials with Schmelzpunkt of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Wärmeformbeständigkeitstemperatur | 195 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 195 °C | dry | ISO 75-1/-2 | 2 MPa | ||
210 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 210 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available | |
Fillers | 10% Glass Fiber |