Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.46 g/cm³ Show Supplier Material materials with Dichte of 1.46 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 1.7 % Show Supplier Material materials with Moisture absorption of 1.7 % | Sim. to ISO 62 |
Wasserabsorption | 23.0 °C | 5.5 % Show Supplier Material materials with Wasserabsorption of 5.5 % | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 11.4 GPa Show Supplier Material materials with Biegemodul of 11.4 GPa | ISO 178 |
Dehnung | 23.0 °C | 3 % Show Supplier Material materials with Dehnung of 3 % | ISO 527-1/-2 |
Elastizitätsmodul | 23.0 °C | 13 GPa Show Supplier Material materials with Elastizitätsmodul of 13 GPa | ISO 527-1/-2 |
Flexural yield strength | 23.0 °C | 285 MPa Show Supplier Material materials with Flexural yield strength of 285 MPa | ISO 178 |
Schlagfestigkeit, Charpy gekerbt | -30.0 °C | 15 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 15 kJ/m² | ISO 179/1eA |
23.0 °C | 21 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 21 kJ/m² | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | -30.0 °C | 90 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 90 kJ/m² | ISO 179/1eU |
23.0 °C | 100 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 100 kJ/m² | ISO 179/1eU | |
Zugfestigkeit | 23.0 °C | 210 MPa Show Supplier Material materials with Zugfestigkeit of 210 MPa | ISO 527-1/-2 |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 220 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 220 °C | ISO 75-1/-2 | |
Heat deflection temperature, 1.80 MPa | 205 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 205 °C | ISO 75-1/-2 | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2E-7 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2E-7 1/K | ISO 11359-1/-2, Parallel |
Schmelzpunkt | 220 °C Show Supplier Material materials with Schmelzpunkt of 220 °C | ISO 11357-1/-3, (10°C/min) | |
Wärmeformbeständigkeitstemperatur | 205 - 220 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 205 - 220 °C | ||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 5E-7 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 5E-7 1/K | ISO 11359-1/-2, Normal |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Fillers | 43% Glass Fiber |