Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.2 g/cm³ Show Supplier Material materials with Dichte of 1.2 g/cm³ | dry | ISO 1183 |
Mechanisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Biegemodul | 0.16 GPa Show Supplier Material materials with Biegemodul of 0.16 GPa | dry | ISO 178 | |
Dehnung | 165 % Show Supplier Material materials with Dehnung of 165 % | dry | ISO 527-1/-2 | |
320 % Show Supplier Material materials with Dehnung of 320 % | dry | ISO 527-1/-2 | ||
Elastizitätsmodul | 0.17 GPa Show Supplier Material materials with Elastizitätsmodul of 0.17 GPa | dry | ISO 527-1/-2 | |
Härte, Shore D | 44 [-] Show Supplier Material materials with Härte, Shore D of 44 [-] | dry | ISO 868 | 3s |
Reißfestigkeit | 74 kN/m Show Supplier Material materials with Reißfestigkeit of 74 kN/m | dry | ISO 34-1; Method B | |
75 kN/m Show Supplier Material materials with Reißfestigkeit of 75 kN/m | dry | ISO 34-1; Method B | ||
Zugfestigkeit | 15 MPa Show Supplier Material materials with Zugfestigkeit of 15 MPa | dry | ISO 527-1/-2 | |
16 MPa Show Supplier Material materials with Zugfestigkeit of 16 MPa | dry | ISO 527-1/-2 | Normal |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzpunkt | 217 °C Show Supplier Material materials with Schmelzpunkt of 217 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Schmelzvolumenflussrate | 230 °C | 12.5 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 12.5 cm³/10min | dry | ISO 1133 | |
Schrumpfung | 1.6 % Show Supplier Material materials with Schrumpfung of 1.6 % | dry | Sim. to ISO 294-4 | Parallel | |
1.6 % Show Supplier Material materials with Schrumpfung of 1.6 % | dry | Sim. to ISO 294-4 | Normal |
Technological properties
Property |
---|