Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.34 g/cm³ Show Supplier Material materials with Dichte of 1.34 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.5 % Show Supplier Material materials with Moisture absorption of 1.5 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Dehnung | 2.5 % Show Supplier Material materials with Dehnung of 2.5 % | dry | ISO 527-1/-2 | |
3.6 % Show Supplier Material materials with Dehnung of 3.6 % | conditioned | ISO 527-1/-2 | ||
120 °C | 4 % Show Supplier Material materials with Dehnung of 4 % | dry | ISO 527-1/-2 | |
160 °C | 20 % Show Supplier Material materials with Dehnung of 20 % | dry | ISO 527-1/-2 | |
180 °C | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-1/-2 | |
200 °C | 30 % Show Supplier Material materials with Dehnung of 30 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 6 GPa Show Supplier Material materials with Elastizitätsmodul of 6 GPa | conditioned | ISO 527-1/-2 | |
8 GPa Show Supplier Material materials with Elastizitätsmodul of 8 GPa | dry | ISO 527-1/-2 | ||
120 °C | 2.1 GPa Show Supplier Material materials with Elastizitätsmodul of 2.1 GPa | dry | ISO 527-1/-2 | |
160 °C | 1.6 GPa Show Supplier Material materials with Elastizitätsmodul of 1.6 GPa | dry | ISO 527-1/-2 | |
180 °C | 1.4 GPa Show Supplier Material materials with Elastizitätsmodul of 1.4 GPa | dry | ISO 527-1/-2 | |
200 °C | 1 GPa Show Supplier Material materials with Elastizitätsmodul of 1 GPa | dry | ISO 527-1/-2 | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 4 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 4 kJ/m² | dry | ISO 179/1eA |
23 °C | 4 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 4 kJ/m² | dry | ISO 179/1eA | |
23 °C | 5.3 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 5.3 kJ/m² | conditioned | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 30 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 30 kJ/m² | dry | ISO 179/1eU |
23 °C | 35 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 35 kJ/m² | dry | ISO 179/1eU | |
23 °C | 40 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 40 kJ/m² | conditioned | ISO 179/1eU | |
Zugfestigkeit | 65 MPa Show Supplier Material materials with Zugfestigkeit of 65 MPa | conditioned | ISO 527-1/-2 | |
95 MPa Show Supplier Material materials with Zugfestigkeit of 95 MPa | dry | ISO 527-1/-2 | ||
120 °C | 25 MPa Show Supplier Material materials with Zugfestigkeit of 25 MPa | dry | ISO 527-1/-2 | |
160 °C | 20 MPa Show Supplier Material materials with Zugfestigkeit of 20 MPa | dry | ISO 527-1/-2 | |
180 °C | 15 MPa Show Supplier Material materials with Zugfestigkeit of 15 MPa | dry | ISO 527-1/-2 | |
200 °C | 12 MPa Show Supplier Material materials with Zugfestigkeit of 12 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Schmelzpunkt | 250 °C Show Supplier Material materials with Schmelzpunkt of 250 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Wärmeformbeständigkeitstemperatur | 190 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 190 °C | dry | ISO 75-1/-2 | 2 MPa | |
225 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 225 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Fillers | 30% Glass Fiber and Mineral Powder |