Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.35 g/cm³ Show Supplier Material materials with Dichte of 1.35 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.5 % Show Supplier Material materials with Moisture absorption of 1.5 % | dry | Sim. to ISO 62 |
Wasserabsorption | 4 % Show Supplier Material materials with Wasserabsorption of 4 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 9 GPa Show Supplier Material materials with Biegemodul of 9 GPa | conditioned | ISO 178 | |
9.1 GPa Show Supplier Material materials with Biegemodul of 9.1 GPa | dry | ISO 178 | ||
Dehnung | 3.3 % Show Supplier Material materials with Dehnung of 3.3 % | dry | ISO 527-1/-2 | |
3.5 % Show Supplier Material materials with Dehnung of 3.5 % | conditioned | ISO 527-1/-2 | ||
120 °C | 15 % Show Supplier Material materials with Dehnung of 15 % | dry | ISO 527-1/-2 | |
140 °C | 14.0 % Show Supplier Material materials with Dehnung of 14.0 % | dry | ISO 527-1/-2 | |
160 °C | 13 % Show Supplier Material materials with Dehnung of 13 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 9.3 GPa Show Supplier Material materials with Elastizitätsmodul of 9.3 GPa | conditioned | ISO 527-1/-2 | |
9.5 GPa Show Supplier Material materials with Elastizitätsmodul of 9.5 GPa | dry | ISO 527-1/-2 | ||
120 °C | 2.8 GPa Show Supplier Material materials with Elastizitätsmodul of 2.8 GPa | dry | ISO 527-1/-2 | |
140 °C | 2.5 GPa Show Supplier Material materials with Elastizitätsmodul of 2.5 GPa | dry | ISO 527-1/-2 | |
160 °C | 2.2 GPa Show Supplier Material materials with Elastizitätsmodul of 2.2 GPa | dry | ISO 527-1/-2 | |
Flexural yield strength | 255 MPa Show Supplier Material materials with Flexural yield strength of 255 MPa | conditioned | ISO 178 | |
285 MPa Show Supplier Material materials with Flexural yield strength of 285 MPa | dry | ISO 178 | ||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 7.5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 7.5 kJ/m² | conditioned | ISO 179/1eA |
-30 °C | 8.5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 8.5 kJ/m² | dry | ISO 179/1eA | |
23 °C | 7.5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 7.5 kJ/m² | conditioned | ISO 179/1eA | |
23 °C | 10 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 10 kJ/m² | dry | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 50 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 50 kJ/m² | conditioned | ISO 179/1eU |
-30 °C | 60 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 60 kJ/m² | dry | ISO 179/1eU | |
23 °C | 50 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 50 kJ/m² | conditioned | ISO 179/1eU | |
23 °C | 65 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 65 kJ/m² | dry | ISO 179/1eU | |
Zugfestigkeit | 170 MPa Show Supplier Material materials with Zugfestigkeit of 170 MPa | conditioned | ISO 527-1/-2 | |
190 MPa Show Supplier Material materials with Zugfestigkeit of 190 MPa | dry | ISO 527-1/-2 | ||
120 °C | 65 MPa Show Supplier Material materials with Zugfestigkeit of 65 MPa | dry | ISO 527-1/-2 | |
140 °C | 55.0 MPa Show Supplier Material materials with Zugfestigkeit of 55.0 MPa | dry | ISO 527-1/-2 | |
160 °C | 45 MPa Show Supplier Material materials with Zugfestigkeit of 45 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Thickness | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|---|
Entflammbarkeit | HB | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes | |
Schmelzpunkt | 250 °C Show Supplier Material materials with Schmelzpunkt of 250 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Wärmeformbeständigkeitstemperatur | 190 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 190 °C | dry | ISO 75-1/-2 | 2 MPa | ||
230 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 230 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Certifications | Food Contact, Drinking Water, Yellow Card Available | |
Fillers | 30% Glass Fiber |