Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.36 g/cm³ Show Supplier Material materials with Dichte of 1.36 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.6 % Show Supplier Material materials with Moisture absorption of 1.6 % | dry | Sim. to ISO 62 |
Wasserabsorption | 6 % Show Supplier Material materials with Wasserabsorption of 6 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 8.4 GPa Show Supplier Material materials with Biegemodul of 8.4 GPa | dry | ISO 178 | |
Dehnung | 3 % Show Supplier Material materials with Dehnung of 3 % | dry | ISO 527-1/-2 | |
5 % Show Supplier Material materials with Dehnung of 5 % | conditioned | ISO 527-1/-2 | ||
Elastizitätsmodul | 7.5 GPa Show Supplier Material materials with Elastizitätsmodul of 7.5 GPa | conditioned | ISO 527-1/-2 | |
9.5 GPa Show Supplier Material materials with Elastizitätsmodul of 9.5 GPa | dry | ISO 527-1/-2 | ||
Flexural yield strength | 250 MPa Show Supplier Material materials with Flexural yield strength of 250 MPa | dry | ISO 178 | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 10 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 10 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 12 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 12 kJ/m² | dry | ISO 179/1eA | |
23 °C | 20 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 20 kJ/m² | conditioned | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 70 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 70 kJ/m² | dry, conditioned | ISO 179/1eU |
23 °C | 80 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 80 kJ/m² | dry | ISO 179/1eU | |
23 °C | 100 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 100 kJ/m² | conditioned | ISO 179/1eU | |
Zugfestigkeit | 140 MPa Show Supplier Material materials with Zugfestigkeit of 140 MPa | conditioned | ISO 527-1/-2 | |
190 MPa Show Supplier Material materials with Zugfestigkeit of 190 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 2e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
7e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 7e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | dry | UL746B | 0.71 mm | ||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | UL746B | 0.71 mm | ||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | dry | UL746B | 0.71 mm | ||
Schmelzpunkt | 260 °C Show Supplier Material materials with Schmelzpunkt of 260 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Wärmeformbeständigkeitstemperatur | 245 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 245 °C | dry | ISO 75-1/-2 | 2 MPa | ||
260 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 260 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 3.5 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.5 [-] | dry | IEC 62631-2-1 | 1MHz |
3.8 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.8 [-] | dry | IEC 62631-2-1 | 100Hz | |
4.6 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4.6 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
11 [-] Show Supplier Material materials with Dielektrizitätskonstante of 11 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Durchschlagfestigkeit | 25 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 25 kV/mm | conditioned | IEC 60243-1 | |
30 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 30 kV/mm | dry | IEC 60243-1 | ||
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | dry, conditioned | IEC 60112 | |
Surface resistivity | 1e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq | conditioned | IEC 62631-3-2 | |
Verlustfaktor | 90 [-] Show Supplier Material materials with Verlustfaktor of 90 [-] | dry | IEC 62631-2-1 | 100Hz |
160 [-] Show Supplier Material materials with Verlustfaktor of 160 [-] | dry | IEC 62631-2-1 | 1MHz | |
1000 [-] Show Supplier Material materials with Verlustfaktor of 1000 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
1400 [-] Show Supplier Material materials with Verlustfaktor of 1400 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schrumpfung | 0.2 % Show Supplier Material materials with Schrumpfung of 0.2 % | dry | Sim. to ISO 294-4 | Parallel |
1.2 % Show Supplier Material materials with Schrumpfung of 1.2 % | dry | Sim. to ISO 294-4 | Normal | |
Specific heat capacity melt | 2170 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 2170 J/(kg·K) | dry | - | |
Thermal conductivity of melt | 0.172 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.172 W/(m·K) | dry | - |
Technological properties
Property | ||
---|---|---|
Application areas | Spatulas and Kitchenware | |
Certifications | Food Contact | |
Fillers | 30% Glass Fiber |