Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.57 g/cm³ Show Supplier Material materials with Dichte of 1.57 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.15 % Show Supplier Material materials with Moisture absorption of 0.15 % | dry | Sim. to ISO 62 |
Wasserabsorption | 0.25 % Show Supplier Material materials with Wasserabsorption of 0.25 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Dehnung | 2.5 % Show Supplier Material materials with Dehnung of 2.5 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 11.5 GPa Show Supplier Material materials with Elastizitätsmodul of 11.5 GPa | dry | ISO 527-1/-2 | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 13 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 13 kJ/m² | dry | ISO 179/1eA |
23 °C | 9.7 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 9.7 kJ/m² | dry | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 65 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 65 kJ/m² | dry | ISO 179/1eU |
23 °C | 65 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 65 kJ/m² | dry | ISO 179/1eU | |
Zugfestigkeit | 155 MPa Show Supplier Material materials with Zugfestigkeit of 155 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Thickness | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|---|
Entflammbarkeit | HB | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes | |
Koeffizient der thermischen Ausdehnung | 3e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 3e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
7e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 7e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Relative temperature index, electrical | 140 °C Show Supplier Material materials with Relative temperature index, electrical of 140 °C | dry | 0.75 mm | UL746B | ||
Relative temperature index, mechanical impact | 130 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 130 °C | dry | 0.75 mm | UL746B | ||
Relative temperature index, mechanical strength | 140 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 140 °C | dry | 0.75 mm | UL746B | ||
Schmelzpunkt | 225 °C Show Supplier Material materials with Schmelzpunkt of 225 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Temperaturleitfähigkeit | 9.01e-08 mm²/s Show Supplier Material materials with Temperaturleitfähigkeit of 9.01e-08 mm²/s | dry | - | |||
Wärmeformbeständigkeitstemperatur | 213 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 213 °C | dry | ISO 75-1/-2 | 2 MPa | ||
224 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 224 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Elektrisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Durchschlagfestigkeit | 30 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 30 kV/mm | dry | IEC 60243-1 |
Kriechstromfestigkeit | 475 V Show Supplier Material materials with Kriechstromfestigkeit of 475 V | dry | IEC 60112 |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Density of melt | 1260 g/cm³ Show Supplier Material materials with Density of melt of 1260 g/cm³ | dry | - | |
Schrumpfung | 0.3 % Show Supplier Material materials with Schrumpfung of 0.3 % | dry | Sim. to ISO 294-4 | Parallel |
1.1 % Show Supplier Material materials with Schrumpfung of 1.1 % | dry | Sim. to ISO 294-4 | Normal | |
Specific heat capacity melt | 1740.0 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 1740.0 J/(kg·K) | dry | - | |
Thermal conductivity of melt | 0.197 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.197 W/(m·K) | dry | - |
Technological properties
Property | ||
---|---|---|
Certifications | Food Contact, Yellow Card Available | |
Fillers | 35% Glass Fiber |